Hostname: page-component-68c7f8b79f-mk7jb Total loading time: 0 Render date: 2025-12-23T10:15:49.317Z Has data issue: false hasContentIssue false

Pop-in phenomenon during nanoindentation in MgO

Published online by Cambridge University Press:  15 September 1999

C. Tromas*
Affiliation:
Laboratoire de Métallurgie Physique (UMR 6630 du CNRS), Université de Poitiers, UFR Sciences, bâtiment SP2MI-Bd 3, Téléport 2, B.P. 179, 86960 Futuroscope Cedex, France
J. Colin
Affiliation:
Laboratoire de Métallurgie Physique (UMR 6630 du CNRS), Université de Poitiers, UFR Sciences, bâtiment SP2MI-Bd 3, Téléport 2, B.P. 179, 86960 Futuroscope Cedex, France
C. Coupeau
Affiliation:
Laboratoire de Métallurgie Physique (UMR 6630 du CNRS), Université de Poitiers, UFR Sciences, bâtiment SP2MI-Bd 3, Téléport 2, B.P. 179, 86960 Futuroscope Cedex, France
J. C. Girard
Affiliation:
Laboratoire de Métallurgie Physique (UMR 6630 du CNRS), Université de Poitiers, UFR Sciences, bâtiment SP2MI-Bd 3, Téléport 2, B.P. 179, 86960 Futuroscope Cedex, France
J. Woirgard
Affiliation:
Laboratoire de Métallurgie Physique (UMR 6630 du CNRS), Université de Poitiers, UFR Sciences, bâtiment SP2MI-Bd 3, Téléport 2, B.P. 179, 86960 Futuroscope Cedex, France
J. Grilhé
Affiliation:
Laboratoire de Métallurgie Physique (UMR 6630 du CNRS), Université de Poitiers, UFR Sciences, bâtiment SP2MI-Bd 3, Téléport 2, B.P. 179, 86960 Futuroscope Cedex, France
Get access

Abstract

During nanoindentation of MgO, a pop-in phenomenon has been observed, that is, an abrupt increase in penetration depth at a critical load. Atomic force microscopy investigations have been performed to characterise the dislocation structure in the vicinity of the indented area. The pop-in has been found to be the first stage of plastic deformation during nanoindentation. This phenomenon is ascribed to the nucleation and further propagation of interstitial loops of dislocations beneath the indenter. A three-dimensional model for a flat ended indenter is developed.

Keywords

Information

Type
Research Article
Copyright
© EDP Sciences, 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

Mura, T., Yamashita, N., Mishima, T., Hirose, Y., Int. J. Eng. Sci. 27, 1 (1989). CrossRef
Tanaka, K., Koguochi, H., Mura, T., Int. J. Eng. Sci 27, 11 (1989). CrossRef
Syed Asif, S.A., Pethica, J.B., Philos. Mag. A 76, 1105 (1997). CrossRef
Page, T.F., Oliver, W.C., Hargue, C.J.M., J. Mater. Res. 7, 450 (1992). CrossRef
Gerberich, W.W., Venkataraman, S.K., Huang, H., Harvey, S.E., Kohlstedt, D.L., Acta Metall. Mater. 43, 1569 (1995). CrossRef
Gerberich, W.W., Nelson, J.C., Anderson, P., Lilleoden, E.T., Wyrobek, J.T., Acta Metall. Mater. 44, 3585 (1996). CrossRef
K.L. Johnson, Contact Mechanics (Cambridge University Press, Cambridge, 1985).
Keh, A.S., J. Appl. Phys. 31, 1538 (1960). CrossRef
Velednitskaya, M.A., Rozhanskii, V.N., Comolova, L.F., Saparin, G.V., Schreiber, J., Brümmer, O., Phys. Stat. Sol. 32, 123 (1975). CrossRef
Loubet, J.L., Georges, J.M., Marchesini, O., Meille, G., J. Lub. Techno. 43, 106 (1984).
Armstrong, R.W., Wu, C.Cm., J. Am. Ceram. Soc. 61, 102 (1978). CrossRef
Chaudhri, M.M., Philos. Mag. A 53, 55 (1986). CrossRef
Woirgard, J., Dargenton, J.-C., Meas. Sci. Technol. 6, 16 (1995). CrossRef
Woirgard, J., Dargenton, J.-C., J. Mater. Res. 12, 2455 (1997). CrossRef
R. De Wit, Solid state physics (Academic Press, 1960), Vol. 10, p. 286.
Duesbery, M.S., Model. Simul. Mater. Sci. Eng. 6, 35-49 (1998). CrossRef
R. De Wit, Solid state physics (Academic Press, 1960), Vol. 10, p. 287.
Sneddon, I.N., Proc. Camb. Phil. Soc. 42, 29 (1946). CrossRef