Hostname: page-component-7f64f4797f-42qgm Total loading time: 0 Render date: 2025-11-09T06:47:29.578Z Has data issue: false hasContentIssue false

Plasma Etching and Surface Analysis of a-SiC:H Films Deposited by Low Temperature Plasma Enhanced Chemical Vapor Deposition

Published online by Cambridge University Press:  22 February 2011

J. H. Thomas III
Affiliation:
David Sarnoff Research Center, Princeton NJ 08543
M. J. Loboda
Affiliation:
Dow Corning Corp. Midland MI 48686
J. A. Seifferly
Affiliation:
Dow Corning Corp. Midland MI 48686
Get access

Abstract

Organosilicon precursors were used to deposit thin films of highly stable amorphous hydrogenated silicon carbide at low temperatures by plasma enhanced chemical vapor deposition. X-ray photoemission and Auger electron spectroscopy were employed to characterize the surface chemistry of air exposed and plasma etched films. Auger analysis of the as-deposited material shows its composition to be constant throughout its depth. RF plasma etching was performed in CF4/O2 and SF6/O2 gas mixtures. Etch rates in these atmospheres are similar to those reported in the literature. After plasma etching, the surface was converted to a highly fluorinated state. In addition to the expected SiC bond, Si-OF bonds were found after plasma etching. Fluorocarbon residue was not produced in this process. Chlorine etching of this low temperature PECVD film is described and is shown to be compatible with standard integrated circuit manufacture processing as an hermetic-like sealant.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Sugiura, J., Lu, W. J., Cadien, K. C. and Steckl, A. J., J. Vac. Sci. Technol. B4, 349 (1986).Google Scholar
2. Pan, W. S. and Steckl, A. J., Mat. Res. Soc. Symp. Proc. 76, 157 (1987).Google Scholar
3. Pan, W. S. and Steckl, A. J., J. Electrochem. Soc. 137, 212 (1990).CrossRefGoogle Scholar
4. Palmour, J. W., Davis, R. F., Astell-Burt, P., and Blackborow, P., Ceramic Trans. 2, 491 (1989).Google Scholar
5. Chandra, Grish, Mat. Res. Soc. Symp. Proc. 203, 97 (1991).Google Scholar
6. Loboda, M. J., Seifferly, J. A. and Dall, F. C., J. Vac. Sci. Technol. A 12(1), (1994), in print.Google Scholar
7. Vossen, J. L., Thomas, J. H. III, Maa, J.-S., Mesker, O. R. and Fowler, G. O., J. Vac. Sci. Technol. A 1, 14521455(1983).Google Scholar
8. Thomas, J. H. III, White, L. K. and Miszkowski, N., Journal of Vacuum Science and Technology A8, 17061711 (1990).CrossRefGoogle Scholar
9. Thomas, J. H. III and Maa, J-S., Applied Physics Letters 43, 859861 (1983).Google Scholar
10. Thomas, J. H. III, and Hammer, L. H., Journal of Vacuum Science and Technology B5, 16171621 (1987).Google Scholar
11. Mayer, T. M., Barker, R. A. and Whitman, L. J., J. Vac. Sci. Technol. 18, 349 (1981).CrossRefGoogle Scholar
12. Mogab, C. J. and Levinstein, H. J., J. Vac. Sci. Technol. 17, 721 (1980).Google Scholar
13. Chang, H-P. and Thomas, J. H. III, Journal of Electron Spectroscopy and related phenomenon 26, 203212 (1982).Google Scholar