Hostname: page-component-68c7f8b79f-fnvtc Total loading time: 0 Render date: 2025-12-20T12:46:56.752Z Has data issue: false hasContentIssue false

On the interface quality of MIS structures fabricated from Atomic Layer Deposition of HfO2, Ta2O5 and Nb2O5−Ta2O5−Nb2O5 dielectric thin films

Published online by Cambridge University Press:  01 February 2011

S. Dueñas
Affiliation:
Departamento de Electricidad y Electrónica, E.T.S.I. Telecomunicación, Campus “Miguel Delibes”, Universidad de Valladolid, 47011 Valladolid., Spain.
H. Castán
Affiliation:
Departamento de Electricidad y Electrónica, E.T.S.I. Telecomunicación, Campus “Miguel Delibes”, Universidad de Valladolid, 47011 Valladolid., Spain.
H. García
Affiliation:
Departamento de Electricidad y Electrónica, E.T.S.I. Telecomunicación, Campus “Miguel Delibes”, Universidad de Valladolid, 47011 Valladolid., Spain.
J. Barbolla
Affiliation:
Departamento de Electricidad y Electrónica, E.T.S.I. Telecomunicación, Campus “Miguel Delibes”, Universidad de Valladolid, 47011 Valladolid., Spain.
K. Kukli
Affiliation:
University of Helsinki, Department of Chemistry, P.O. Box 55, FIN-00014 Helsinki, Finland. University of Tartu, Institute of Experimental Physics and Technology, Tähe 4, EE-51010 Tartu, Estonia.
M. Ritala
Affiliation:
University of Helsinki, Department of Chemistry, P.O. Box 55, FIN-00014 Helsinki, Finland.
M. Leskelä
Affiliation:
University of Helsinki, Department of Chemistry, P.O. Box 55, FIN-00014 Helsinki, Finland.
Get access

Abstract

A study of metal-insulator-semiconductor (MIS) structures based on atomic layer deposited HfO2, Ta2O5 and Nb2O5−Ta2O5−Nb2O5 thin films is presented. Our attention was focussed on interface quality and defect density in the dielectric. Interface states as well as defects inside the insulator bulk were measured by using capacitance-voltage (C-V), deep level transient spectroscopy (DLTS) and conductance transient (G-t) techniques. Nb2O5−Ta2O5−Nb2O5 based capacitors exhibit the highest interface state density, whereas the minimum is obtained for HfO2. Conductance transients are not observed in Al/HfO2/SiO2/Si stacks, thus indicating that disordered induced gap states (DIGS) are not present in these structures. We also observed that post-metallization annealing in forming gas diminishes the trap interface density at the expense of increasing DIGS in the Al/HfO2/Si cases.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Harris, H., Choi, K., Metha, N., Chandolu, A., Biswas, N., Kipshidze, G., Nikishin, S., Gangopadhyay, S., and Temkin, H., Appl. Phys. Lett. 81, 1065 (2002).Google Scholar
2. Lai, Y. S., Chen, K. J., and Chen, J. S., J. Electrochem. Soc. 149, 163 (2002)Google Scholar
3. Kukli, K., Ritala, M., and Leskelä, M., J. Appl. Phys. 86, 5656 (1999).Google Scholar
4. Kukli, K., Ritala, M., Leskelä, M., Sajavaara, T., Keinonen, J., Gilmer, D., Bagchi, S., amd Prabhu, L., J. Non-Cryst. Solids 303, 35 (2002).Google Scholar
5. Ritala, M. and Leskelä, M., “Deposition and Processing of Thin Film Materials”, Handbook of Thin Films Materials Vol. 1, ed. Nalwa, H. S. (Academic, San Diego, 2002), p. 104.Google Scholar
6. Dueñas, S., Peláez, R., Castán, H., Pinacho, R., Quintanilla, L., Barbolla, J., Mártil, I., and González-Díaz, G., Appl. Phys. Lett. 71, 826 (1997).Google Scholar
7. He, L., Hasegawa, H., Sawada, T., Sawada, T., and Ohno, H., J. Appl. Phys. 63, 2120 (1988).Google Scholar