Hostname: page-component-857557d7f7-nhjpk Total loading time: 0 Render date: 2025-11-20T16:34:45.773Z Has data issue: false hasContentIssue false

Nucleation and Growth During Tungsten Atomic Layer Deposition on Oxide Surfaces

Published online by Cambridge University Press:  21 March 2011

S. M. George
Affiliation:
Department of Chemistry and Biochemistry, University of Colorado, Boulder, CO 80309 Department of Chemistry and Biochemistry, University of Colorado, Boulder, CO 80309 Steven.George@Colorado.Edu
J.W. Elam
Affiliation:
Department of Chemistry and Biochemistry, University of Colorado, Boulder, CO 80309
R.K. Grubbs
Affiliation:
Department of Chemistry and Biochemistry, University of Colorado, Boulder, CO 80309
C.E. Nelson
Affiliation:
Department of Chemistry and Biochemistry, University of Colorado, Boulder, CO 80309
Get access

Abstract

Nucleation and growth has been studied during tungsten (W) atomic layer deposition (ALD) on oxide surfaces. Auger electron spectroscopy (AES) was utilized to examine the deposition of W during the sequential (A) WF6 and (B) Si2H6 reaction cycles that define W ALD. The AES results displayed an initial nucleation period of ∼10 AB cycles to deposit one tungsten monolayer on SiO2. Subsequently, the W and Si AES signals grew and oscillated dramatically versus WF6 and Si2H6 exposures. The increase in the W AES signal in the growth region was consistent with a W ALD growth rate of 3.5 Å per AB cycle. An examination of the oxygen and tungsten AES signals versus AB cycles indicated that W ALD displayed nearly ideal “layer-by-layer”, Frank- van der Merwe growth after the nucleation period. On Al2O3, the AES results displayed a much shorter nucleation period for W ALD. Only 3 AB cycles were required to deposit one tungsten monolayer. Subsequently, the tungsten film grew at a rate of 3.6 Å per AB cycle. The initial nucleation period and growth mechanism during ALD are important because they will affect the roughness of the resulting ALD film.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

[1] George, S. M., Ott, A. W., Klaus, J. W., J. Phys. Chem. 100, 13121 (1996).Google Scholar
[2] Kodas, T., Hampden-Smith, M., The Chemistry of Metal CVD (VCH, New York, 1994).Google Scholar
[3] Klaus, J.W., Ferro, S.J. and George, S.M., Thin Solid Films 360, 145 (2000).Google Scholar
[4] Elam, J.W., Nelson, C.E., Grubbs, R.K. and George, S.M., Thin Solid Films 386, 41 (2000).Google Scholar
[5] Sneh, O. and George, S.M., J. Vac. Sci. Technol. A 13, 493 (1995).Google Scholar
[6] Ott, A. W., Klaus, J. W., Johnson, J. M., George, S. M., Thin Solid Films 292, 135 (1997).Google Scholar
[7] NIST Electron Inelastic-Mean-Free-Path Database, Version 1.0, Prepared by Powell, C.J. and Jablonski, A., U.S. Department of Commerce, National Institute of Standards and Technology, Gaithersburg, MD, September 1999.Google Scholar
[8] Elam, J.W., Nelson, C.E., Grubbs, R.K. and George, S.M., Surf. Sci. 479, 121 (2001).Google Scholar
[9] Tokutaka, H., Nishimori, K., Takashima, K., Surf. Sci. 133, 547 (1983).Google Scholar
[10] Ossicini, S., Memeo, R., Ciccacci, F., J. Vac. Sci. Technol. A 3, 387 (1985).Google Scholar