Hostname: page-component-68c7f8b79f-7mrzp Total loading time: 0 Render date: 2025-12-20T20:25:40.491Z Has data issue: false hasContentIssue false

Nanoindentation Studies of Yield Point Phenomena on Gold Single Crystals

Published online by Cambridge University Press:  15 February 2011

S. G. Corcoran
Affiliation:
Naval Research Laboratory, Code 6177, Washington, DC 20375–5342
R. J. Colton
Affiliation:
Naval Research Laboratory, Code 6177, Washington, DC 20375–5342
E. T. Lilleodden
Affiliation:
University of Minnesota, Department of Chemical Engineering and Materials Science, Minneapolis, MN 55455–0132
W. W. Gerberich
Affiliation:
University of Minnesota, Department of Chemical Engineering and Materials Science, Minneapolis, MN 55455–0132
Get access

Abstract

Nanoindentation studies often show an instantaneous displacement-excursion in the loaddisplacement curve. This anomaly is generally associated with a surface contamination effect, dislocation emission, a phase transition, or an oxide break-through event. The determination of which effect is operative is often difficult when investigating oxide covered surfaces. We have performed a detailed nanoindentation study on clean, flame annealed single-crystal Au thus eliminating the effects of a surface oxide or contamination layer. Multiple displacement excursions were observed exhibiting a new phenomenon of “staircase” yielding. Owing to the fact that our radius of contact is more than an order of magnitude smaller than the average dislocation spacing expected for well annealed Au, the excursions are explained in terms of multiple dislocation nucleation events on parallel slip bands. Indentation data were taken on Au (111), (110), and (100) single crystal surfaces.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Tangyunyong, P., Thomas, R.C., Houston, J.E., Michalske, T.A., Crooks, R.M. and Howard, A.J., Phys. Rev. Lett., 71, 3319 (1993).Google Scholar
2. Oliver, W.C. and Pharr, G.M., J. Mater. Res., 7, 1564 (1992).Google Scholar
3. Venkataraman, S.K., Kohlstedt, D.L. and Gerberich, W.W., J. Mater. Res., 8, 685 (1993).Google Scholar
4. Gerberich, W.W., Venkataraman, S.K., Huang, H., Harvey, S.E. and Kohlstedt, D.L., Acta Metall. Mater. 43(4), 1569 (1995).Google Scholar
5. Lilleodden, E., Bonin, W., Nelson, J. and Gerberich, W.W., J. Mater. Res. Commun., 10 (9), 2162 (1995).Google Scholar
6. Gerberich, W.W., Nelson, J.C., Lilleodden, E.T., Anderson, P., and Wyrobek, J.T., Acta. Metall. Mater., in press.Google Scholar
7. Corcoran, S.G., Colton, R.J., Lilleodden, E.T., Gerberich, W.W., in preparation.Google Scholar
8. Gane, N. and Bowden, F.P., J. Appl. Phys., 39, 1432 (1968).Google Scholar
9. Pethica, J.B. and Tabor, D., Surf. Sci., 89, 182 (1979).Google Scholar
10. Sneddon, I.N., Int. J. Engng. Sci, 3, 47 (1965).Google Scholar
11. An average of the values compiled in: Single Crystal Elastic Constants and Calculated Aggregate Properties: A Handbook, edited by Gene, Simmons and Herbert, Wang (MIT Press, Cambridge, MA, 1971).Google Scholar
12. The indentation-modulus values were calculated by Hoehn, Joel, UMN, based on a model developed originally by Joost, Vlassak and Nix, W., Stanford U.Google Scholar