Hostname: page-component-68c7f8b79f-m4fzj Total loading time: 0 Render date: 2025-12-19T19:25:23.881Z Has data issue: false hasContentIssue false

Nanoindentation of Poly (Methyl Methacrylate)

Published online by Cambridge University Press:  17 March 2011

Michael J. Adams
Affiliation:
Unilever Research Port Sunlight, Bebington, Wirral, CH63 3JW, U.K.
David M. Gorman
Affiliation:
Unilever Research Port Sunlight, Bebington, Wirral, CH63 3JW, U.K.
Simon A. Johnson
Affiliation:
Unilever Research Port Sunlight, Bebington, Wirral, CH63 3JW, U.K.
Get access

Abstract

For the indentation of an elastic-plastic homogeneous half-space with a pyramidal indenter, the load theoretically increases with the square of the total penetration depth. Experimental data are presented in the current paper that demonstrate the validity of this relationship for an organic polymer and a Berkovich indenter, provided that appropriate account is taken of the tip defect and viscoplasticity. It is also shown that a simple analytical solution exists for the ratio of the contact depth to the total penetration depth. These findings assist in identifying procedures for obtaining the rate-dependent mechanical properties of thin polymer coatings or polymeric materials with depth-dependent mechanical properties.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Loubet, J.L., Georges, J.M. and Meille, G., in Microindentation Techniques in Materials Science and Engineering, edited by Blau, P.J. and Lawn, B.R. (ASTM, Philadelphia,1986) pp. 7289.Google Scholar
2. Malzbender, J., With, G. de and Toonder, J. den, J. Mater. Res., 15, 12091212 (2000).Google Scholar
3. Malzbender, J. and With, G. de, Surface and Coatings Technol., 127, 266273 (2000).Google Scholar
4. Hainsworth, S.V., Chandler, H.W. and Page, T.F., J. Mater. Res., 11, 19871995 (1996).Google Scholar
5. Oliver, W.C. and Pharr, G.M., J. Mater. Res., 7, 15641583 (1992).Google Scholar
6. Lucas, B.N. and Oliver, W.C., Metall. Mater. Trans. A – Phys. Metall. Mater. Sci., 30, 601610 (1999).Google Scholar
7. Grau, P., Meinhard, H. and Mosch, S., in Fundamentals of Nanoindentation and Nanotribology, edited by Moody, N.R., Gerberich, W.W., Burnham, N. and Baker, S.P., (Mater. Res. Soc. Proc. 522, Warrendale, PA, 1998) pp. 153158.Google Scholar
8. Hochstetter, G., Jimenez, A. and Loubet, J.L., J. Macromol. Sci.-Phys., B38, 681692 (1999).Google Scholar
9. Berthoud, P., G'Sell, C. and Hiver, J.-M., J. Phys. D: Appl. Phys., 32, 29232932 (1999).Google Scholar