Nanoindentation of a Layered Crystal Structure Oxide

Published online by Cambridge University Press:  10 February 2011

M. P. Shemkunas
Affiliation:
Science and Engineering of Materials Program, Arizona State University, Tempe, AZ 85287
W. T. Petuskey
Affiliation:
Department of Chemistry and Biochemistry, Arizona State University, Tempe, AZ 85287
Get access

Abstract

Nanoindentation was performed on layered structure materials to determine values for stiffness and hardness perpendicular to the layers. In order to establish the validity of this technique for anisotropic materials, layered minerals with known elastic constants were tested, including brucite and muscovite mica. A layered ceramic oxide of interest, KCa2Nb3O10, was also investigated. A Berkovich diamond tip was used to carry out the indentations. Indents were made on atomically flat surfaces of crystals, as observed in-situ with an atomic force microscope. Analysis of load versus displacement data showed that the elastic constant C 33 for muscovite and brucite agreed to within five percent of literature values. In the case of KCa2Nb3O10, average values of 57.0 GPa for C 33 and 3.8 GPa hardness were obtained.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Sambasivan, S. (private communication).Google Scholar
2. Dion, M., Ganne, M. and Tournoux, M., Mat. Res. Bull. 16, p. 1429 (1981).Google Scholar
3. Jacobson, A. in Chemical Physics of Intercalation II, edited by P., Bernier, et al., Plenum Press, New York, 1993, pp. 117139.Google Scholar
4. Oliver, W. C. and Pharr, G. M., J. Mater. Res. 7, pp. 15641583 (1992).Google Scholar
5. Hysitron Inc., Triboscope manual.Google Scholar
6. McNeil, L. E. and Grimsditch, M., J. Phys.: Condens. Matter 5, pp. 16811690 (1993).Google Scholar
7. Xia, X., Weidner, D. J. and Zhao, H., Amer. Mineralogist 83, pp. 6874, (1998).Google Scholar
8. Bahr, D. F., Hoehn, J. W., Moody, N. R. and Gerberich, W. W., Acta Mater. 45, pp. 51635175, (1997).Google Scholar