Nanoindentation and Nanowear Studies of Thin Carbon Coatings

Published online by Cambridge University Press:  10 February 2011

Ashok V. Kulkarni
Affiliation:
Hysitron Inc. 2010 E.Hennepin Ave, Minneapolis, MN 55413
Jerzy T. Wyrobek
Affiliation:
Hysitron Inc. 2010 E.Hennepin Ave, Minneapolis, MN 55413
Zhenghong Qiant
Affiliation:
Department of Electric Engineering, University of Minneapolis, MN 55455
John M. Siverstent
Affiliation:
Department of Electric Engineering, University of Minneapolis, MN 55455
Jack Judyt
Affiliation:
Department of Electric Engineering, University of Minneapolis, MN 55455
Get access

Abstract

Thin film magnetic disks and head-sliders require protective overcoats, usually some form of carbon, to guard the magnetic elements against corrosion and wear and to provide long interface durability. The mechanical properties of these coatings are important for assessing their tribological performance. In this paper we present the results of nanomechanical properties of amorphous carbon (a-C) and nitrogenated carbon (CN) films deposited on Si(100). a-C and CN films were deposited on silicon by Facing Target Sputtering (FTS) technique. The elemental composition and bond characterization of a-C and CN films have been determined by X-ray Photoelectron spectroscopy (XPS). Nanoindentation experiments were performed using Hysitron Triboscope® in the load range of 10–200 μN, using a sharp 90° 3-sided pyramidal diamond tip ( 50 ± 10 nm radius). Hardness and Young's modulus of elasticity were determined from the load-displacement data. Nanowear studies were performed on the 10 and 20 nm a-C and CN films to determine the critical load. Below the critical load no significant wear is observed. Above the critical load however, the wear increases sharply. Abrasive wear seems to be the cause of the sharp increase in wear depth in case of a-C film. From the above observation, CN films exhibit excellent mechanical properties owing to its superior hardness property.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Wallace, B.L., Bell Syst. Tech. J., vol 30, pp. 11451173, Oct. 1951.Google Scholar
2.Bhushan, B., Tribology and Mechanics of magnetic Storage Devices, Springer, New York 1990.Google Scholar
3.Grill, A., Horng, C.T., Meyerson, B.S., Patel, V.V. and Russak, M.A., Magnetic head slider having a protective coating thereon, US patent 5, 159,508, Oct 27, 1992.Google Scholar
4.Ganapathi, S.K. and Reiner, T.A., ASME J. Tribol., vol.117, pp. 8693, 1995.Google Scholar
5.Catherine, Y., Preparation techniques for diamond-like carbon, in Clausing, R.E., Horton, L.L., Angus, J.C., and Koidl, P. (eds.), Diamond and Diamind-like Films and Coatings, Plenum, New York, 1991, pp. 193227.Google Scholar
6.Cuomo, J.J., Pappas, D.L., Bruley, J., Doyle, J.P., Saenger, K.L., J.Appl. Phys., vol.70, pp. 17061711, 1991.Google Scholar
7.Wang, G., Strojny, A., Siversten, J.M., Judy, J.H., and Gerberich, W.W., Mater. Res. Soc. Proc., vol.426, pp. 345351, 1997.Google Scholar
8.Bogy, D.B. and Jiang, Zhaoguo, Mater. Res. Soc. Proc., vol.356, pp. 737748, 1995.Google Scholar
9.Lu, C.–J., Bogy, D.B. and Kaneko, R., ASME J. Tribol., vol.116, pp. 175180, 1995.Google Scholar
10.Jiang, Z., Lu, C.–J., Bogy, D.B. and Miyamoto, T., Wear, vol. 181–183, pp. 777783, 1995.Google Scholar
11.Bhushan, B., Gupta, B.K. and Azarian, M.H., Wear, vol. 181–183, pp. 743758, 1995.Google Scholar
12.Naoe, M., Yamanaka, S. and Hoshi, Y., IEEE Trans. Magn. MAG–16, pp. 646648, 1982.Google Scholar
13.Bhushan, B., kulkarni, A.V., Bonin, W. and Wyrobek, J.T., Philos. Mag. A, vol 74, pp. 11171128, 1996.Google Scholar
14.Oliver, W.C. and Pharr, G.M., J. Mater. Res., vol.7, pp. 15641583, 1992.Google Scholar
15.Kumar, S. and Tansley, T.L., Thin Solid Films, vol.256, pp. 4447, 1995.Google Scholar
16.Niu, C., Lu, Y.Z., and Lieber, C.M., Science, vol.261, pp. 334, 1993.Google Scholar