Molecular Dynamics Simulations of Nanoindentation of Silicon Nitride

Published online by Cambridge University Press:  15 February 2011

Phillip Walsh
Affiliation:
Concurrent Computing Laboratory for Materials Simulation, Department of Physics & Astronomy and Department of Computer Science, Louisiana State University, Baton Rouge, LA, 70803-4001
Andrey Omeltchenko
Affiliation:
Concurrent Computing Laboratory for Materials Simulation, Department of Physics & Astronomy and Department of Computer Science, Louisiana State University, Baton Rouge, LA, 70803-4001
Hideaki Kikuchi
Affiliation:
Concurrent Computing Laboratory for Materials Simulation, Department of Physics & Astronomy and Department of Computer Science, Louisiana State University, Baton Rouge, LA, 70803-4001
Rajiv K. Kalia
Affiliation:
Concurrent Computing Laboratory for Materials Simulation, Department of Physics & Astronomy and Department of Computer Science, Louisiana State University, Baton Rouge, LA, 70803-4001
Aiichiro Nakano
Affiliation:
Concurrent Computing Laboratory for Materials Simulation, Department of Physics & Astronomy and Department of Computer Science, Louisiana State University, Baton Rouge, LA, 70803-4001
Priya Vashishta
Affiliation:
Concurrent Computing Laboratory for Materials Simulation, Department of Physics & Astronomy and Department of Computer Science, Louisiana State University, Baton Rouge, LA, 70803-4001
Get access

Abstract

This is a report of work in progress on 10 million atom Molecular Dynamics (MD) simulations of nanoindentation of crystalline and amorphous silicon nitride (Si3N4). Nanoindentation is used to determine mechanical properties of extremely thin films such as hardness and elastic moduli. We report load-displacement curves for several Si3N4 configurations using an idealized non-deformable indenter and analyze the local stress distributions in the vicinity of the indenter tip. Preliminary results for surface adhesion using Si3N4 for both tip and substrate are also reported.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Pollock, H.M., in Friction Lubrication, and Wear Technology, edited by Blau, P.J., (ASM Metals Handbook 18, 1992), p. 419.Google Scholar
2. Burnham, N.A. and Colton, R.J., J. Vac. Sci. Technol. A 7(4), p. 2906 (1989).Google Scholar
3. Landman, Uzi and Luedtke, W.D., J. Vac. Sci. Technol. B 9(2), p. 414 (1990).Google Scholar
4. Omeltchenko, Andrey, Nakano, Aiichiro, Tsuruta, Kenji, Kalia, Rajiv K., and Vashishta, Priya, Advances in Metal and Semiconductor Clusters 4, p. 263 (1998).Google Scholar
5. Landman, Uzi, Luedtke, W.D., Burnham, Nancy A., Colton, Richard J., Science 248, p. 454 (1990).Google Scholar
6. Harrison, J.A., White, C.T., Colton, R.J., and Brenner, D.W., Surface Science 271, p. 57(1992).Google Scholar
7. Tuckerman, M. and Berne, B.J., J. Chem. Phys. 97(3): p. 1990 (1992)Google Scholar
8. Vashishta, P., Kalia, R.K., Rino, J.P., and Ebbsjo, I., Phys. Rev. B 41(17), p. 12197 (1990)Google Scholar
9. Vashishta, P., Kalia, R.K., and Ebbsjb, Ingvar, Phys. Rev. Lett. 75(5), p. 858 (1995)Google Scholar
10. Loong, C.K., Vashishta, P., Kalia, R.K., and Ebbsjo, I., Europhys. Lett. 31(4), p. 201 (1995)Google Scholar
11. Omeltchenko, A., Nakano, A., Kalia, R.K., and Vashishta, P., Europhys. Lett. 33(9), p.667 (1996).Google Scholar