Mechanical Property Data for Coated Systems-The Prospects for Measuring “Coating Only” Properties using Nanoindentation

Published online by Cambridge University Press:  15 February 2011

S. V. Hainsworth
Affiliation:
Materials Division, University of Newcastle upon Tyne, Newcastle upon Tyne, NEI 7RU, UK.
T. F. Page
Affiliation:
Materials Division, University of Newcastle upon Tyne, Newcastle upon Tyne, NEI 7RU, UK.
Get access

Abstract

One of the critical aspects of assessing the properties of coated systems is the prospect of being able to measure the properties of the coating in isolation of the substrate. This has led to an increase in the use of continuously-recording indentation techniques (or nanoindentation techniques) for assessing the mechanical properties of coated systems since they can be used to measure the materials response to contact deformation at a scale relevant to the coating thickness. This paper presents the results of a new method for analysing the nanoindentation loading curves for coated systems. The analysis of the loading curve uses the relationship P = Km δ2 which describes the indenter displacement, δ, in terms of the applied load P. For each material, Km can be predicted from its modulus E and hardness H. One result is that if either of E or H is known, then the other may be calculated from the experimental loading curve. Further, the method has the potential to differentiate between the responses of the coating only, the coating and substrate in combination, and that dominated by the substrate once the load has become sufficient for cracking of the coating such that it no longer plays a significant role in supporting the applied load. In many cases, careful analysis of the loading curves allows the displacement ranges associated with these regimes to be identified. This is shown to be a powerful experimental tool for the interpretation of the mechanical properties of coated systems.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Page, T.F. and Hainsworth, S.V., Surface Coatings and Technology 61 201208 (1993)Google Scholar
2. Page, T.F., these proceedings, (1996)Google Scholar
3. Doemer, M.F. and Nix, W.D., J. Mater. Res. 1 601609 (1986)Google Scholar
4. Oliver, W.C. and Pharr, G. M, J. Mater. Res. 7 15641583 (1992)Google Scholar
5. Swain, M.V. and Mencík, J., Thin Solid Films 253 204211 (1994)Google Scholar
6. Hainsworth, S.V., Chandler, H.W. and Page, T.F., accepted for J. Mater. Res., 1996 Google Scholar
7. Loubet, J.L., Georges, J. M. and Meille, J., in Microindentation Techniques in Materials Science and Enpaneering Eds. Blau, P.J. and Lawn, B. R., American Society for Testing and Materials, Philadelphia, 1986, 7289 Google Scholar
8. Hainsworth, S.V., unpublished workGoogle Scholar
9. Pharr, G.M. and Oliver, W.C., MRS Bulletin, 17 2833 (1992)Google Scholar
10. Yu, H.Y., Sanday, S.C. and Rath, B.B., J. Mech. Phys. Solids 38 745764 (1990)Google Scholar
11. Williams, J.A., Engineering Tribology, Oxford University Press, 1994, p. 95 Google Scholar