The Mechanical Properties of Thin Polymer Films from Nanoindentation

Published online by Cambridge University Press:  01 February 2011

F R Jones
Affiliation:
Ceramics and Composites Laboratory, Department of Engineering Materials, The University of Sheffield, Sir Robert Hadfield Building, Mappin Street, Sheffield, S1 3JD, UK.
S A Hayes
Affiliation:
Ceramics and Composites Laboratory, Department of Engineering Materials, The University of Sheffield, Sir Robert Hadfield Building, Mappin Street, Sheffield, S1 3JD, UK.
Get access

Abstract

The thermomechanical properties of thermoset polymeric materials are shown to be suitable for detecting relevant degradative processes in the matrix of a fibre composite. In space environments, the surface of the material will be modified first because of the diffusion of the active molecules. Nanoindentation has been shown to be capable of determining changes in viscoelastic properties of thin polymer films and at surfaces of bulk material. The Hysitron Triboscope has been used to characterise an epoxy resin and polycyanurate in dynamic and static scanning modes. Dynamic nanoindentation has been shown to provide a full description of the viscoelastic response. Progress has been made in analysing static indentation for time dependence.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Oliver, W. C. and Pharr, S. M., J. Mater. Res., 7, 1564 (1992).Google Scholar
2. Ahn, H., Klimek, K. S. and Rie, K. T., Surf. Coat. Technol. 174–175, 1225 (2003)Google Scholar
3. Phani, A. R., Kranowski, J. E. and Nainaparampil, J. J., J. Mater, Res. 17, 1261 (2002).Google Scholar
4. Du, B., Tsui, O. K. C., Zhang, Q. and He, T., Langmuir 17, 3286 (2001).Google Scholar
5. van Landingham, M. R., Villarrubia, J. S., Guthrie, W. F. and Meyers, G. F., Macromol. Symp. 167, 15 (2001).Google Scholar
6. Nowicki, M., Richter, A., Wolf, B. and Kaczmarek, H., Polymer 44, 6599 (2003).Google Scholar
7. Hayes, S A, Goruppa, A A and Jones, F R J. Mater. Res. 19, (2004).Google Scholar
8. Karad, S. K., Attwood, D. and Jones, F. R., Composites A, 33, 1665 (2002).Google Scholar