Measurement of Electrical Charge During Nanoindentation of Ferroelectric Thin Films

Published online by Cambridge University Press:  17 March 2011

M. Algueró
Affiliation:
Department of Materials. Queen Mary, University of London. Mile End Road, London E1 4NS, United Kingdom
A.J. Bushby
Affiliation:
Department of Materials. Queen Mary, University of London. Mile End Road, London E1 4NS, United Kingdom
M.J. Reece
Affiliation:
Department of Materials. Queen Mary, University of London. Mile End Road, London E1 4NS, United Kingdom
Get access

Extract

Electrical charge transients have been measured during the nanoindentation of lanthanum modified lead titanate ferroelectric thin films. Using the spherical indenter as the top electrode, the films were locally poled. The films were then reindented at the exact same positions. The origin of the charge released is discussed in terms of piezoelectricity and depolarisation. The depolarisation must have been produced by a stress induced ferroelastic domain reorientation. Current intensity transients recorded during indentation showed a distinct maximum. This maximum corresponded to a force at which the depolarisation rate was a maximum. This provides the basis to define a coercive indentation force, and then a coercive indentation stress.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

[1] Spearing, S.M., “Materials issues in microelectromechanical systems (MEMS)”, Acta Mater. 48 179 (2000).Google Scholar
[2] Itoh, T. and Suga, T., “Self-excited force-sensing microcantilevers with piezoelectric thin films for dynamic scanning force microscopy”. Sensors and Actuators A 54 477 (1996).Google Scholar
[3] Racine, G.A., Muralt, P. and Dubois, M.A., “Flexural-standing-wave elastic force motor using ZnO and PZT thin film on micromachined silicon membranes for wristwatch applications”. Smart Mater. Struct. 7 404 (1998).Google Scholar
[4] Kholkin, A.L., Colla, E.L., Tagantsev, A.K. and Taylor, D.V., “Fatigue of piezoelectric properties in Pb(Zr,Ti)O3 films”. Appl. Phys. Lett. 68(18) 2577 (1996).Google Scholar
[5] Algueró, M., Kholkin, A.L., Calzada, M.L. and Pardo, L., “Dependence of functional properties on processing in sol-gel (Pb,La)TiO3 thin films”. Appl. Phys. A 71 195 (2000).Google Scholar
[6] Brooks, K.G., Reaney, I.M., Klissurska, R., Huang, Y., Bursill, L. and Setter, N., “Orientation of rapid thermally annealed lead zirconate thin films on (111) Pt substrates”. J. Mater. Res. 9(10) 2540 (1994).Google Scholar
[7] Watanabe, S., Fujiu, T. and Fuji, T., “Effect of poling on piezoelectric properties of lead zirconate titanate thin films formed by sputtering”. Appl. Phys. Lett. 66(12) 1481 (1995).Google Scholar
[8] Cao, H. and Evans, A.G., “Nonlinear deformation of ferroelectric ceramics”. J. Am. Ceram. Soc. 76(4) 890 (1993).Google Scholar
[9] Poyato, R., Calzada, M.L., Ricote, J., Pardo, L. and Willing, B., “Spontaneous pyro and piezoelectricity of sol-gel La modified lead titanate thin films”. To be published in Integrated Ferroelectrics.Google Scholar
[10] Giannakopoulos, A.E. and Suresh, S., “Theory of indentation of piezoelectric materials”. Acta Mater. 47(7) 2153 (1999).Google Scholar
[11] Sridhar, S., Giannakopoulous, A.E., Suresh, S. and Ramamurty, U., “Electrical response during indentation of piezoelectric materials: A new method for material characterisation”. J. Appl. Phys. 85(1) 380 (1999).Google Scholar
[12] Setter, N. and Waser, R., “Electroceramic materials”. Acta Mater. 48 151 (2000).Google Scholar
[13] Lawn, B.R.. “Indentation of ceramics with spheres: A century aftr Hertz”. J. Am. Ceram. Soc. 81(8) 1977 (1998).Google Scholar