In-situ Infrared Absorption Monitoring of Atomic Layer Deposition of Metal Oxides on Functionalized Si and Ge Surfaces

Published online by Cambridge University Press:  01 February 2011

Min Dai
Affiliation:
mindai@physics.rutgers.edu, Rutgers University, Chemistry and Chemical Biology, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States
Jinhee Kwon
Affiliation:
jinhee@physics.rutgers.edu, Rutgers University, Physics and Astronomy, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States
Ming-Tsung Ho
Affiliation:
mtho@physics.rutgers.edu, Rutgers University, Physics and Astronomy, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States
Yu Wang
Affiliation:
ywang4@tulane.edu, Rutgers University, Physics and Astronomy, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States
Sandrine Rivillon
Affiliation:
rivillon@physics.rutgers.edu, Rutgers University, Chemistry and Chemical Biology, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States
Meng Li
Affiliation:
mengli@physics.rutgers.edu, Rutgers University, Physics and Astronomy, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States
Yves Jean Chabal
Affiliation:
yves@agere.rutgers.edu, Rutgers University, Chemistry and Chemical Biology, Laboratory for Surface Modification, 136 Frelinghuysen Road, Piscataway, NJ, 08854, United States, (732) 445-8248, (732) 445-4991
Marek Boleslawski
Affiliation:
mboleslawski@sial.com, SAFC Hitech, 5485 County Road V, Sheboygan Falls, WI, 53085, United States
Get access

Abstract

The nature of the interface between Si and Ge substrates and high-k dielectrics often controls the performance of MOSFET devices. Precleaning and/or chemical functionalization of the surfaces can dramatically affect the formation of an interfacial layer. We have used in-situ IR spectroscopy to probe the relevant interfaces during ALD growth for a variety of surface treatments, including H- and Cl-termination, and nitridation. This paper focuses on understanding of the mechanisms for interfacial SiO2 (or GeOx) formation during HfO2 growth using tetrakis-ethylmethylamidohafnium (TEMAH) as the metal precursor and water or ozone as the oxygen precursor. We find that impurities arising from incomplete ligand elimination during growth (e.g. OH for H2O processing and CO- and NO-containing species for O3 processing) are incorporated into the HfO2 film during growth. Upon annealing, most of these species react, but can also migrate to the interface. Nitridation of Si and Ge surfaces will in general prevent SiO2 or GeOx formation but can also affect the growth rate.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1.International Technology Roadmap for Semiconductors web site: http://www.itrs.net/ Google Scholar
2. Wilk, G. D., Wallace, R. M., and Anthony, J. M., J. Appl. Phys. 89, 5243 (2001).Google Scholar
3. Kang, C. Y., Rhee, S. J., Choi, C. H., Akvar, M. S., Zhang, M., Lee, T., Ok, I., and Lee, J. C., Appl. Phys. Lett. 86, 012901 (2005).Google Scholar
4. Xuan, Y., Ye, P. D., Lin, H. C., and Wilk, G. D., Appl. Phys. Lett. 89, 132103 (2006).Google Scholar
5. Ritala, M. and Leskela, M., in Handbook of Thin Film Materials, Vol. 1, edited by Nalwa, H. S. (Academic, New York, 2002).Google Scholar
6. Higashi, G. S., Chabal, Y. J., Trucks, G. W., and Raghavachari, K., Appl. Phys. Lett. 56, 656 (1990).Google Scholar
7. Rivillon, S., Chabal, Y. J., Webb, L. J., Michalak, D. J., Lewis, N. S., Halls, M. D., and Raghavachaari, K., J. Vac. Sci. Technol. A 23, 1100 (2005).Google Scholar
8. Tachuchi, H. and King, T. J., Appl. Phys. Lett. 83, 788 (2003).Google Scholar
9. Rivillon, S. and Chabal, Y. J., Appl. Phys. Lett. 87, 253101 (2005).Google Scholar
10. Wang, Y., Dai, M., Ho, M,-T., Wielunski, L. S., and Chabal, Y. J., Appl. Phys. Lett. 90, 022906 (2007).Google Scholar