Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Bruemmer, S.M.
Olszta, M.J.
Toloczko, M.B.
and
Thomas, L.E.
2013.
Linking Grain Boundary Microstructure to Stress Corrosion Cracking of Cold-Rolled Alloy 690 in Pressurized Water Reactor Primary Water.
Corrosion,
Vol. 69,
Issue. 10,
p.
953.
Lozano-Perez, Sergio
Dohr, Judith
Meisnar, Martina
and
Kruska, Karen
2014.
SCC in PWRs: Learning from a Bottom-Up Approach.
Metallurgical and Materials Transactions E,
Vol. 1,
Issue. 2,
p.
194.
Meisnar, Martina
Lozano-Perez, Sergio
Moody, Michael
and
Holland, James
2014.
Low-energy EDX – A novel approach to study stress corrosion cracking in SUS304 stainless steel via scanning electron microscopy.
Micron,
Vol. 66,
Issue. ,
p.
16.
Meisnar, Martina
Vilalta-Clemente, Arantxa
Gholinia, Ali
Moody, Michael
Wilkinson, Angus J.
Huin, Nicolas
and
Lozano-Perez, Sergio
2015.
Using transmission Kikuchi diffraction to study intergranular stress corrosion cracking in type 316 stainless steels.
Micron,
Vol. 75,
Issue. ,
p.
1.
Meisnar, Martina
Vilalta-Clemente, Arantxa
Moody, Michael
Arioka, Koji
and
Lozano-Perez, Sergio
2016.
A mechanistic study of the temperature dependence of the stress corrosion crack growth rate in SUS316 stainless steels exposed to PWR primary water.
Acta Materialia,
Vol. 114,
Issue. ,
p.
15.
Kuang, Wenjun
Song, Miao
and
Was, Gary S.
2018.
Insights into the stress corrosion cracking of solution annealed alloy 690 in simulated pressurized water reactor primary water under dynamic straining.
Acta Materialia,
Vol. 151,
Issue. ,
p.
321.
Kuang, Wenjun
Song, Miao
Parish, Chad M.
and
Was, Gary S.
2019.
Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors.
p.
535.
Kuang, Wenjun
Song, Miao
Parish, Chad M.
and
Was, Gary S.
2019.
Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors.
p.
535.
Saravanan, Naganand
Karamched, Phani S
Liu, Junliang
Rainasse, Claire
Scenini, Fabio
and
Lozano-Perez, Sergio
2020.
Using local GND density to study SCC initiation.
Ultramicroscopy,
Vol. 217,
Issue. ,
p.
113054.
de Andrade, Ageo Meier
Geers, Christine
Chen, Jiaxin
and
Panas, Itai
2024.
Stress-corrosion cracking sensitization by hydrogen upon oxidation of nickel-base alloys by water – An experiment-guided first-principles study.
Journal of Nuclear Materials,
Vol. 595,
Issue. ,
p.
155044.
Chang, Hai
Yang, Chensheng
Huang, Feifei
Zhang, Hongbo
Wen, Lei
Li, Wenchao
Ai, Yibo
and
Jin, Ying
2024.
Study of Stress-Corrosion Cracking on 304 Stainless Steel by Wedge Opening Loading Method and Acoustic Emission Technique.
Journal of Materials Engineering and Performance,
Lozano-Perez, Sergio
Roberts, Ed
Karamched, Phani
and
Shen, Zhao
2024.
Quantification of SCC mechanisms in austenitic alloys under PWR primary water conditions.
Corrosion Reviews,
Vol. 42,
Issue. 5,
p.
565.