Hostname: page-component-68c7f8b79f-wfgm8 Total loading time: 0 Render date: 2025-12-23T12:09:20.287Z Has data issue: false hasContentIssue false

Determination of Plastic Properties of Polycrystalline Metallic Materials by Nanoindentation – Experiments and Finite Element Simulations

Published online by Cambridge University Press:  01 February 2011

Karsten Durst
Affiliation:
Materials Science and Engineering, University Erlangen - Nürnberg D-91058 Erlangen, Germany
Björn Backes
Affiliation:
Materials Science and Engineering, University Erlangen - Nürnberg D-91058 Erlangen, Germany
Mathias Göken
Affiliation:
Materials Science and Engineering, University Erlangen - Nürnberg D-91058 Erlangen, Germany
Get access

Abstract

The determination of plastic properties of metallic materials by nanoindentation requires the analysis of the indentation process and the evaluation methods. Particular effects on the nanoscale, like the indentation size effect or piling up of the material around the indentation, need to be considered. Nanoindentation experiments were performed on conventional grain sized (CG) as well as on ultrafine-grained (UFG) copper and brass. The indentation experiments were complemented with finite element simulations using the monotonic stress-strain curve as input data. All indentation tests were carried out using cube-corner and Berkovich geometry and thus different amount of plastic strain was applied to the material, according to Tabors theory. We find an excellent agreement between simulations and experiments for the UFG materials from which a representative strain of εB ≈ 0.1 and εcc ≈ 0.2 is determined. With these data, the slope of the stress-strain curve is predicted for all materials down to an indentation depth of 800 nm.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Tabor, D., The hardness of metals, Clarendon Press, Oxford (1951).Google Scholar
2. Cheng, Y., Cheng, C., Surf. Coat. Technol. 133 417 (2000).Google Scholar
3. Atkins, A.G., Tabor, D., J. Mech. Phys. Solids 13 149 (1965).Google Scholar
4. Nix, W.D., Gao, H., J. Mech. Phys. Solids 46 441 (1998).Google Scholar
5. Oliver, W.C., Pharr, G.M., J. Mater. Res. 7 1564 (1992).Google Scholar
6. Bolshakov, A., Pharr, G.M., J. Mater. Res. 13 1049 (1998).Google Scholar
7. Durst, K., Göken, M., Vehoff, H., J. Mater. Res. 19 85 (2004).Google Scholar
8. Durst, K., Backes, B., Göken, M., submitted to Scripta Mat. (2005).Google Scholar
9. Joslin, D.L., Oliver, W.C., J. Mater. Res. 5 123 (1990).Google Scholar