Hostname: page-component-857557d7f7-h6shg Total loading time: 0 Render date: 2025-11-25T12:42:39.948Z Has data issue: false hasContentIssue false

Creep Strengthening of Iron-Nickel-Base Superalloy for High-Stress Condition by Cubo-Octahedral Nanoparticles Precipitation

Published online by Cambridge University Press:  07 July 2014

Ming-Yen Li
Affiliation:
New Materials Research & Development Department, China Steel Corporation, 1 Chung Kang Road, Hsiao Kang, Kaohsiung 81233, Taiwan, R.O.C.
Shih-Ming Kuo
Affiliation:
New Materials Research & Development Department, China Steel Corporation, 1 Chung Kang Road, Hsiao Kang, Kaohsiung 81233, Taiwan, R.O.C.
Yeong-Tsuen Pan
Affiliation:
New Materials Research & Development Department, China Steel Corporation, 1 Chung Kang Road, Hsiao Kang, Kaohsiung 81233, Taiwan, R.O.C.
Get access

Abstract

Under a creep condition of relatively intense stress, dispersive precipitation of TiC nanoparticles could be promptly brought out within the austenite grain when the iron-nickel-base superalloy was fabricated through the specific production of the ingenious alloy design, applicable electro-slag remelting and high-temperature solution-anneal developed in this study. Both the TiC and coexistent M23C6 precipitates are cubo-octahedral in shape, remaining the cube-to-cube orientation relationship and coherent {111}carbide/γ and {100}carbide/γ interphase interface with the austenite, which bring about the dispersion-strengthening effect so that the time to rupture for the present alloy could be increased by 1.8 times of magnitude relative to the commercial creep-resistant product of the same grade. The improved creep property can be attributed to the mechanism that the nanometer-scale intragranular TiC and submicron intergranular M23C6 can act as pinning points for individual dislocations and grain boundaries, respectively, resulting in the raised Orowan strengthening and suppressed grain boundary sliding. Since the strengthening media found in this study are thermally stable and able to emerge readily prior to the formation of γ’ phase at the temperature range studied, this work suggested an improved grade of heat resistant alloy for applications in a relatively harsh environment that the creep lifetime might be shorter than the incubation period of the common strengthening phase for superalloys.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2014 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Betteridge, W., Krefeld, R., Krockel, H., Lloyd, S.J., Van de Voorde, M.,, in Alloy 800, edited by Vivante, C. (North Holland Publishing, New York, 1978).Google Scholar
Ren, W., in A Review of Alloy 800H for Applications in the Gen IV Nuclear Energy Systems, PVP2010–25727, Bellevue Washington (2010).CrossRefGoogle Scholar
Li, M.Y., Pan, Y.T., Hong, I.T.Kuo, S.M., Proceedings of the 2012 Annual Conference of the Materials Research Society-Taiwan, Yunlin, Taiwan, Nov. 23-24th, 2012, pp.26312634.Google Scholar
Jones, W.B. and Allen, R.M., Met. Trans. A, 13, 637 (1982).CrossRefGoogle Scholar
Taneike, M., Abe, F., Sawada, K., Nature, 424, 294 (2003).CrossRefGoogle Scholar
Orlová, A., Milička, K., Čadek, J., Mat. Sci. Eng. A, 50, 221 (1981), and references cited therein.CrossRefGoogle Scholar
Chen, C.Y., Internal Report TS-101001 in China Steel Corporation, 2012.Google Scholar