Hostname: page-component-5b777bbd6c-cp4x8 Total loading time: 0 Render date: 2025-06-19T08:11:55.713Z Has data issue: false hasContentIssue false

Area Selective Atomic Layer Deposition by Soft Lithography

Published online by Cambridge University Press:  01 February 2011

Rong Chen
Affiliation:
rongchen@stanford.edu, Stanford University, Chemistry, 381 North-South Mall, Stauffer II, Rm219, Stanford University, Stanford, California, 94305-5025, United States
David W. Porter
Affiliation:
porterd@stanford.edu, Stanford University, Dept. of Chemical Engineering, Stanford, CA, 94305, United States
Hyoungsub Kim
Affiliation:
hsubkim@skku.edu, Stanford University, Dept. of Materials Science and Engineering, Stanford, CA, 94305, United States
Paul C. McIntyre
Affiliation:
pcm1@stanford.edu, Stanford University, Dept. of Materials Science and Engineering, Stanford, CA, 94305, United States
Stacey F. Bent
Affiliation:
sbent@stanford.edu, Stanford University, Dept. of Chemical Engineering, Stanford, CA, 94305, United States
Get access

Abstract

Area selective HfO2 thin film growth through atomic layer deposition (ALD) has been achieved on octadecyltrichlorosilane (ODTS) patterned Si substrates. Patterned hydrophobic self-assembled monolayers (SAMs) were first transferred to Si substrates by micro-contact printing. Using hafnium-tetrachloride or tetrakis(dimethylamido) hafnium(IV) and water as ALD precursors, amorphous HfO2 layers were then grown selectively on the SAM-free regions of the surface where native hydroxyl groups nucleate growth from the vapor phase. The HfO2 pattern was readily observed through scanning electron microscopy and scanning Auger imaging, demonstrating that soft lithography is a simple and promising method to achieve area selective ALD. To evaluate the selectivity, the resolution of the soft lithography based method was compared with that of area selective ALD of HfO2 by selective surface modification of patterned silicon oxide obtained using long-time SAM exposure. It was found that the selective surface modification showed much higher spatial resolution and selectivity, an observation consistent with previous studies indicating that highly ordered and densely packed ODTS films were important to achieve complete deactivation.

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Packan, P., Science 285, 2079 (2000).Google Scholar
2 Wilk, G. D. and Wallace, R. M, Appl. Phys. Lett. 76, 112 (2000).Google Scholar
3 Kang, L., Jeon, Y., Onishi, K., Lee, B. H., Qi, W-J., Nieh, R., Gopalan, S., and Lee, J. C., Dig. Tech. Pap. - Symp. VLSI. Technol.; Jun 13-15; Honolulu, HI, USA, 44 (2000).Google Scholar
4 Biercuk, M. J., Monsma, D. J., Marcus, C. M., Becker, J. S., and Gordon, R. G., Appl. Phys. Lett. 83 (12), 2405 (2003).Google Scholar
5 Chen, R., Kim, H., McIntyre, P. C., and Bent, S. F., Appl. Phys. Lett. 84, 4017 (2004).Google Scholar
6 Lee, J. P. and Sung, M. M., J. Am. Chem. Soc. 126, 28 (2004).Google Scholar
7 Park, K. J., Doub, J. M., Gougousi, T., and Parsons, G. N., Appl. Phys. Lett. 86 (5), 51903 (2005).Google Scholar
8 Park, M. H., Jang, Y. J., Sung-Suh, H. M., and Sung, M. M., Langmuir 20, 2257 (2004).Google Scholar
9 Yan, M., Koide, Y., Babcock, J. R., Markworth, P. R., Belot, J. A., Marks, T. J., and Chang, R. P. H., Appl. Phys. Lett. 79, 1709 (2001).Google Scholar
10 Ulman, A., Chem. Rev. 96, 1533 (1996).Google Scholar
11 Chen, R., Kim, H., McIntyre, P. C., Porter, D. W., and Bent, S. F., Appl. Phys. Lett. 86 (19), 191910 (2005).Google Scholar
12 Xia, Y. and Whitesides, G. M., Angew. Chem., Int. Ed. 37, 550 (1998).Google Scholar
13 Chen, R., Kim, H., McIntyre, P. C., and Bent, S. F., Chem. Mater. 17 (3), 536 (2005).Google Scholar