Hostname: page-component-68c7f8b79f-gnk9b Total loading time: 0 Render date: 2025-12-23T16:07:13.819Z Has data issue: false hasContentIssue false

Variations of Internal Stresses within a Rafted Superalloy during High Temperature Mechanical Testing: An in situ XRD Study

Published online by Cambridge University Press:  14 March 2013

Alain Jacques
Affiliation:
Institut Jean Lamour – SI2M (UMR CNRS – UdL 7198, labex DAMAS) parc de Saurupt, 54000 Nancy, France
Laura Dirand
Affiliation:
Institut Jean Lamour – SI2M (UMR CNRS – UdL 7198, labex DAMAS) parc de Saurupt, 54000 Nancy, France
Thomas Schenk
Affiliation:
Institut Jean Lamour – SI2M (UMR CNRS – UdL 7198, labex DAMAS) parc de Saurupt, 54000 Nancy, France
Jean Philippe Chateau-Cornu
Affiliation:
Institut Jean Lamour – SI2M (UMR CNRS – UdL 7198, labex DAMAS) parc de Saurupt, 54000 Nancy, France
Olivier Ferry
Affiliation:
Institut Jean Lamour – SI2M (UMR CNRS – UdL 7198, labex DAMAS) parc de Saurupt, 54000 Nancy, France
Pierre Bastie
Affiliation:
LIPhy (UMR CNRS –UJF N° 5588) 140 Avenue de la Physique - BP 87, 38402 Saint Martin d’Hères, France
Get access

Abstract

Modeling of the mechanical behavior of a two-phased material, even with a simple microstructure such as a single crystal superalloy remains a difficult task, for lack of phase specific experimental data. The combination of Three Crystal Diffractometry with high energy synchrotron radiation and in situ experiments can give access to such data in real time. A few examples are given on load transfer between phases, dislocation densities, and the stress – strain behavior of a phase.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2013

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Veron, M., Brechet, Y. and Louchet, F., Acta Mater. 44, 3633 (1996).CrossRefGoogle Scholar
Sarosi, P. M. et al. ., Acta Mater. 55, 2509 (2007).CrossRefGoogle Scholar
Mompiou, F. and Caillard D, D., Mater. Sci. Eng A 483484, 143 (2008).CrossRefGoogle Scholar
Viguier, B., Touratier, F. and Andrieu, E., Philos. Mag. 91, 4427 (2011).CrossRefGoogle Scholar
Jacques, A., Diologent, F., Caron, P. and Bastie, P., Mater. Sci. Eng A 483484, 568 (2008).CrossRefGoogle Scholar
Kuhn, H. A., Biermann, H., Ungar, T. and Mughrabi, H. Acta Metall. 39, 2783 (1991).CrossRefGoogle Scholar
Royer, A., Bastie, P., Bellet, D. and Strudel, J. L., Philos. Mag. A 72 669 (1995).CrossRefGoogle Scholar
Biermann, H., Strehler M, M. and Mughrabi, H., Metall. Mater. Trans. A 27, 1003(1996).CrossRefGoogle Scholar
Jacques, A. and Bastie, P., Philos. Mag. A 83, 26, 3005(2003).CrossRefGoogle Scholar
Dirand, L. et al. ., Philos. Mag. (2012) (in press).Google Scholar
Spätig, P., Bonneville, J. and Martin, J.-L., Mater. Sci. Eng. 167, 1–2, 7379 (1993).CrossRefGoogle Scholar