Hostname: page-component-7f64f4797f-l842n Total loading time: 0 Render date: 2025-11-05T02:31:44.437Z Has data issue: false hasContentIssue false

Probing Silicate/Sapphire Interfaces with AFM and Nanoindentation

Published online by Cambridge University Press:  15 February 2011

E. T. Lilleodden
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, carter@cems.umn.edu
A. V. Zagrebelny
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, carter@cems.umn.edu
S. Ramamurthy
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, carter@cems.umn.edu
C. B. Carter
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, carter@cems.umn.edu
Get access

Abstract

A nanoindentation study of a calcium-aluminosilicate/α-alumina system is described. Thinfilms of CaAl2Si2O8 glass were deposited on α-alumina single crystals of {1120} and {1102} orientations by pulsed-laser deposition. These samples were then subjected to a heat treatment causing the glass to crystallize and to dewet the sapphire surface. A nanoindentation device retrofitted on an atomic force microscope was employed to probe the mechanical properties of the samples. It uniquely enables the characterization of sub-micron features such as the dewet crystallites which necessitate small displacements and exact positioning of the indenter. Strong dependencies on the crystallographic anisotropy were observed in the morphology, but less so on the mechanical properties. In addition, displacement-excursions were observed and are explained in terms of yielding in the substrate.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Weiderhorn, S.M., in Ultra-Fine Grain Ceramics, Edited by Burke, J.J., Reed, N.L. and Weiss, V., Syracuse University Press, NY (1970).Google Scholar
2. O'Donnell, H.L., Readey, M.J. and Kovar, D., J. Am. Ceram. Soc. 78(4) 849 (1995).Google Scholar
3. Padture, N.P. and Chan, H.M., J. Mater. Res., 26 2711–5 (1991).Google Scholar
4. Zagrebelny, A.V., Lilleodden, E.T., Ramamurthy, S. and Carter, C.B., Mater.Res.Soc. Symp. Proc. 401 (1995).Google Scholar
5. Mallamaci, M. P., ”Interfaces Between Alumina and Silicate-glass Films”, Ph. D. Thesis, Cornell University, Ithaca, NY (1995).Google Scholar
6. Hysitron, Inc. (Minneapolis, MN).Google Scholar
7. Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7(6) 1564 (1992).Google Scholar
8. Nix, W.D., Met. Trans. 20A 2217 (1989).Google Scholar
9. Gerberich, W.W., Nelson, J.C., Lilleodden, E.T., Anderson, P. and Wyrobek, J.T., Acta Met. In Press (1996).Google Scholar
10. Page, T.F., Oliver, W.C. and McHargue, C.J., J. Mater. Res. 7(2) 450 (1992).Google Scholar
11. Johnson, K.L., Contact Mechanics, Cambridge University Press, NY (1985).Google Scholar