Plasma-assisted Atomic Layer Deposition of TiN Films at low Deposition Temperature for High-aspect Ratio Applications

Published online by Cambridge University Press:  01 February 2011

S.B.S. Heil
Affiliation:
Eindhoven University of Technology, Dept. of Applied Physics, P.O. Box 513, 5600 MB Eindhoven, The Netherlands
E. Langereis
Affiliation:
Eindhoven University of Technology, Dept. of Applied Physics, P.O. Box 513, 5600 MB Eindhoven, The Netherlands
F. Roozeboom
Affiliation:
Philips Research, Prof. Holstlaan 4, 5656 AA Eindhoven, The Netherlands 3Delft University of Technology, DIMES-ECTM, P.O. Box 5053, 2600 GB Delft, The Netherlands
A. Kemmeren
Affiliation:
Philips Research, Prof. Holstlaan 4, 5656 AA Eindhoven, The Netherlands 3Delft University of Technology, DIMES-ECTM, P.O. Box 5053, 2600 GB Delft, The Netherlands
N.P. Pham
Affiliation:
Philips Research, Prof. Holstlaan 4, 5656 AA Eindhoven, The Netherlands 3Delft University of Technology, DIMES-ECTM, P.O. Box 5053, 2600 GB Delft, The Netherlands
P.M. Sarro
Affiliation:
Philips Research, Prof. Holstlaan 4, 5656 AA Eindhoven, The Netherlands 3Delft University of Technology, DIMES-ECTM, P.O. Box 5053, 2600 GB Delft, The Netherlands
M.C.M. van de Sanden
Affiliation:
Eindhoven University of Technology, Dept. of Applied Physics, P.O. Box 513, 5600 MB Eindhoven, The Netherlands
W.M.M. Kessels
Affiliation:
Eindhoven University of Technology, Dept. of Applied Physics, P.O. Box 513, 5600 MB Eindhoven, The Netherlands
Get access

Abstract

A plasma-assisted atomic layer deposition (PA-ALD) process of titanium nitride (TiN) using TiCl4 precursor dosing and H2/N2 plasma exposure is presented. In situ spectroscopic ellipsometry revealed a growth rate at 400 °C of ∼0.7 A/cycle independent of precursor dosing. Varying the plasma exposure time changed the stoichiometry [N]/[Ti] of the films within the range ∼0.93-1.15. At 100 °C a relatively low chlorine impurity level (∼2 at. %) and low resistivity (∼200 νΔcm) were obtained for a ∼45 nm thick film. The growth rate was found to be considerably lower (∼0.3 Å/cycle) at this temperature. Using TEM imaging we found that PAALD TiN films can be deposited conformally in 20:1 aspect-ratio features (1.5 Êm width) but that the step coverage still needs to be improved, probably by a prolonged plasma exposure step.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

[1] Elers, K.E., Saanila, V., Soininen, P.J., Li, W.M., Kostamo, J.T., Haukka, S., Juhanoja, J., and Besling, W.F.A., Chem. Vap. Deposition 8, 149 (2002).Google Scholar
[2] Kim, H. and Rossnagel, S.M., J. Vac. Sci. Technol. A 20, 802 (2002).Google Scholar
[3] Rossnagel, S.M., Sherman, A., and Turner, F., J. Vac. Sci. Technol. B 18, 2016 (2000).Google Scholar
[4] Kim, H., Cabral, C. Jr, Lavoie, C., and Rossnagel, S.M., J. Vac. Sci. Technol. B 20, 1321 (2002).Google Scholar
[5] Kim, H., J. Vac. Sci. Technol. B 21, 2231 (2003).Google Scholar
[6] Heil, S.B.S., Langereis, E., Kemmeren, A., Roozeboom, F., Sanden, M.C.M. van de, and Kessels, W.M.M., submitted for publication.Google Scholar
[7] Greer, F., Fraser, D., Coburn, J.W., and Graves, D.B., J. Vac. Sci. Technol A. 21, 96 (2003).Google Scholar
[8] Roozeboom, F., Kemmeren, A., Verhoeven, J., Heuvel, E. van den, Kretschman, H., and Frié, T., Mat. Res. Soc. Symp. Proc. 783, 157 (2004).Google Scholar