Physical and Electrical Properties of Al2O3, HfO2, and their Alloy Films Prepared by Atomic Layer Deposition for 65nm CMOS Gate Dielectric

Published online by Cambridge University Press:  11 February 2011

Takaaki Kawahara
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Kazuyoshi Torii
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Seiichi Fukuda
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Takeshi Maeda
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Atsushi Horiuchi
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Hiroyuki Ito
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Akiyoshi Muto
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Yoshitake Kato
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Hiroshi Kitajima
Affiliation:
Semiconductor Leading Edge Technologies, Inc. (Selete), 34, Miyukigaoka, Tsukuba-shi, Ibaraki-ken, 305–8501, Japan Phone: +81–298–63–6316 Fax: +81–298–56–3482 E-mail: kawahara@selete.co.jp
Get access

Abstract

We have investigated physical and electrical properties of Al2O3, HfO2, and their alloy films deposited on 300mm Si wafers by Atomic Layer Deposition (ALD). It is found that Al2O3 films are not crystallized even after the heat treatment of 1050°C, while HfO2 films are already crystallized even after a-Si deposition (530°C). The crystallization temperature can be higher by adding Al2O3 to HfO2. It is confirmed by in-plane XRD and plane views of TEM that HfAlOx films with lower Hf content (Hf/(Hf+Al) <30%) are amorphous without phase separation after annealing at 1050°C and 5sec. The dependences of equivalent oxide thicknesses (EOT) on the physical thicknesses of Al2O3, HfAlOx (Hf/(Hf+Al)∼22%), and HfO2 films in poly-silicon gate capacitors indicate that those dielectric constants k are ∼9, 14, and 23, respectively. The gate dielectric with EOT of 1.5nm and the leakage current density J g of 3mA/cm2 can be fabricated with 2nm-thick HfAlOx (22%) film.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

[1] Buchanan, D.A., Gusev, E.P., Cartier, E., et al.: Tech. Digest IEDM, p. 223 (2000)Google Scholar
[2] Lee, J. H., Koh, K., Lee, N. I., Cho, M. H., Kim, Y. K., et al.: Tech. Digest IEDM, p. 645 (2000)Google Scholar
[3] Torii, K., Shimamoto, Y., Saito, S., Tonomura, O., et al.: VLSI Symp., p. 188 (2002)Google Scholar
[4] Kang, L., Onishi, K., Jeon, Y., Lee, B.H., Kang, C., et al.: Tech. Digest IEDM, p. 35 (2000)Google Scholar
[5] Lee, J.H., Kim, Y.S., Jung, H.S., Lee, J.H., Lee, N.I., et al.: VLSI Symp., p. 84 (2002)Google Scholar
[6] Yamaguchi, T., Satake, H., Fukushima, N., and Toriumi, A.: Tech. Digest IEDM, p. 19 (2000)Google Scholar
[7] Maeda, T., Fukuda, S., and Kato, Y., IWGI 2001, Tokyo, p210.Google Scholar
[8] Saito, S., Torii, K., Hiratani, M., and Onai, T., IEEE Electron Device Letters, 23 (2002) 348.Google Scholar