The liquidus temperature (TL) often limits the loading of high-level waste in glass through the constraint that TL must be at least 100°C below the temperature at which the glass viscosity is 5 Pa-s. In this study, values of TL for spinel primary crystalline phase were measured as a function of glass composition. The test glasses were based on high-iron Hanford Site tank wastes. All studied glasses precipitated spinel (Ni,Fe,Mn)(Cr,Fe)2O4 as the primary crystalline phase. TL was increased by additions of Cr2O3, NiO, Al2O3, Fe2O3, MgO, and MnO; while Li2O, Na2O, B2O3, and SiO2 had a negative effect. Empirical mixture models were fitted to data.