Evaluation of Pb Precursors for Liquid Injection Atomic Layer Deposition of Pb(ZrxTi1-x)O3 Thin Films

Published online by Cambridge University Press:  26 February 2011

Takayuki Watanabe
Affiliation:
t.watanabe@fz-juelich.de, Research Center Juelich, Leo-Brandt-Str., Juelich, NRW, 52425, Germany
Susanne Hoffmann-Eifert
Affiliation:
su.hoffmann@fz-juelich.de, Research Center Juelich, Germany
Cheol Seong Hwang
Affiliation:
cheolsh@plaza.snu.ac.kr, Seoul National University, Korea, Republic of
Rainer Waser
Affiliation:
waser@iwe.rwth-aachen.de, Research Center Juelich, Germany
Get access

Abstract

Pb(DPM)2 and Pb(TMOD)2 dissolved in ethylcyclohexane were evaluated as precursors for future atomic layer deposition (ALD) of Pb(Zr,Ti)O3 films. PbO films were deposited by a liquid injection atomic layer deposition on Pt-covered Si substrates at different deposition temperature and precursor volume per cycle. Pb(DPM)2 and Pb(TMOD)2 started thermal decomposition at deposition temperature of around 270°C and 320°C, respectively. Against increasing Pb(DPM)2 injection at 240°C, the deposition rate of PbO films saturated at around 1 Å/cycle, but kept increasing at 300°C, which is above the thermal decomposition temperature. The deposition rate of PbO films at 240°C dropped to a constant value with enough purge time after precursor injection and reactant supply. A saturated deposition rate of PbO films was also observed for Pb(TMOD)2 below the thermal decomposition temperature. However, the saturation behavior observed for Pb(TMOD)2 was slower and the saturated growth rate was higher comparing to Pb(DPM)2. In addition, the film thickness of the PbO films had an apparent gradient over the substrates. These results indicate that Pb(DPM)2 shows more reactive and stable chemisorption comparing to Pb(TMOD)2 for the self-limiting growth rate.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Shimizu, M., Hyodo, S., Fujisawa, H., Niu, H., and Shiosaki, T., Jpn. J. Appl. Phys. 36, 5808 (1997).Google Scholar
2 Fujisawa, H., Kita, K., Shimizu, M., and Niu, H., Jpn. J. Appl. Phys. 40, 5551 (2001).Google Scholar
3 Hwang, C. S., No, S. Y., Park, J., Kim, H. J., Cho, H. J., Han, Y. K., and Oh, K. Y., J. Electrochem. Soc. 149, G185 (2002).Google Scholar
4 Niinistö, L., Päiväsaari, J., Niinistö, J., Putkonen, M., and Nieminen, M., Phys. Stat. Sol. (a) 201, 1443 (2004).Google Scholar
5 ICDD No. 38-1477.Google Scholar
6 ICDD No. 05-0561.Google Scholar