Determination of the Real Indenter Shape for Nanoindentation/Nanotribology Tests by Surface Metrological and Analytical Investigations

Published online by Cambridge University Press:  17 March 2011

S. Enders
Affiliation:
NRC Innovation Centre, Surface Technology-Tribology Group, Vancouver, Canada
P. Grau
Affiliation:
Martin-Luther-University Halle-Wittenberg, FB Physik-ExPh I, D-06108 Halle, Germany
H. M. Hawthorne
Affiliation:
NRC Innovation Centre, Surface Technology-Tribology Group, Vancouver, Canada
Get access

Abstract

In this paper a critical comparison of different kinds of surface metrological methods like atomic force microscopy (AFM), scanning electron microscopy (SEM) and optical interferometric profilometry is made, as well as analytical investigations based on both Hertz and Sneddon theories of pure elastic contact, to qualify the real indenter shape function. The results obtained show the advantages and disadvantages of the respective methods by describing a rounded indenter tip.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

[1] Herrmann, K., Haschke, K., Pohlenz, F., Seemann, R., Menelao, F., presented at the MicroMat 2000, Berlin,2000 ( to be published)Google Scholar
[2] Pethica, J.B., Oliver, W.C.: Mat.Res.Soc. Symp.Proc. 130, 13, (1989)Google Scholar
[3] Sneddon, I.N.: Int.J.Enging.Sci. 3, 47, (1965)Google Scholar
[4] Bolshakov, A., Oliver, W.C., Pharr, G.M.: Mat.Res.Soc. Symp.Proc. 356, 675, (1995)Google Scholar
[5] Grau, P., Meinhard, H., Mosch, S.: Mat.Res.Soc. Symp. Proc. 522, 153,(1998)Google Scholar
[6] WYCO Surface Profilers, Technical Reference ManualGoogle Scholar