Correlating Small Angle Scattering Spectra to Electrical Resistivity Changes in a Nickel-base Superalloy

Published online by Cambridge University Press:  01 February 2011

Ricky L Whelchel
Affiliation:
gtg359w@mail.gatech.edu, Georgia Institute of Technology, Materials Science and Engineering, Atlanta, Georgia, United States
V. Siva Kumar G. Kelekanjeri
Affiliation:
sivakumar.vkg@gmail.com, Georgia Institute of Technlogy, Materials Science and Engineering, Atlanta, Georgia, United States
Rosario Gerhardt
Affiliation:
rosario.gerhardt@mse.gatech.edu, Georgia Institute of Technology, Materials Science and Engineering, Atlanta, Georgia, United States
Jan Ilavsky
Affiliation:
ilavsky@aps.anl.gov, Argonne National Laboratory, X-Ray Division, Argonne, Illinois, United States
Ken C. Littrell
Affiliation:
littrellkc@ornl.gov, Oak Ridge National Laboratory, High Flux Isotope Reactor, Oak Ridge, Tennessee, United States
Get access

Abstract

Waspaloy specimens aged at 800°C from 0.5h to 88.5h were evaluated via small angle neutron scattering (SANS), ultra small angle X-ray scattering (USAXS), electrical resistivity, and SEM. The average γ' precipitate size and volume fraction, obtained from modeling the small angle scattering data, was used to calculate a figure of merit of electron scattering. This figure of merit is designed to correlate the electron scattering ability of the material to the precipitate microstructure. The USAXS data shows a secondary precipitate population at smaller diameters that is absent from the SANS data, since the SANS measurements were not obtained at high enough values of Q. It is believed that this secondary population makes the USAXS-derived figure of merit more sensitive to the actual measured resistivity response than the SANS-derived values; however, the SANS derived primary precipitate sizes are believed to more accurate due to a larger sample volume.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 White, R. J. Fisher, S. B. Miller, K. M. and Swallow, G. A.Resistometric Study of Aging in Nimonic Alloys (1). PE16,” Journal of Nuclear Materials, vol. 52, pp. 5158, 1974.Google Scholar
2 Kelekanjeri, V. S. K. G. Moss, L. K. Gerhardt, R. A. and Ilavsky, J.Quantification of the Coarsening Kinetics of γ' Precipitates in Waspaloy Microstructures with Different Prior Homogenizing Treatments,” Acta Materialia, vol. 57, pp. 46584670, 2009.Google Scholar
3 Whelchel, R. L. Kelekanjeri, V. S. K. G. Gerhardt, R. A. and Ilavsky, J. “Effect of Aging Treatment on the Microstructure and Resistivity of a Nickel Base Superalloy1,” Metallurgical and Materials Transactions A, Submitted for publication.Google Scholar
4 Ilavsky, J. Jemian, P. R. Allen, A. J. Zhang, F. Levine, L. E. and Long, G. G.Ultrasmall-angle X-ray scattering at the Advanced Photon Source,” Journal of Applied Crystallography, vol. 42, pp. 469479, 2009.Google Scholar
5 Littrell, Ken C. private communication.Google Scholar
6 Ilavsky, J. and Jemian, P. R.Irena: tool suite for modeling and analysis of small-angle scattering,” Journal of Applied Crystallography, vol. 42, pp. 347353, 2009.Google Scholar
7 Kelekanjeri, V. S. K. G. and Gerhardt, R. A.A closed-form solution for the computation of geometric correction factors for four-point resistivity measurements on cylindrical specimens,” Measurement Science and Technology, vol. 19, pp. 025701025712, 2008.Google Scholar