Controlling Area-Selective Atomic Layer Deposition of HfO2 Dielectric by Self-assembled Monolayers

Published online by Cambridge University Press:  28 July 2011

Rong Chen
Affiliation:
Department of Chemistry, Stanford University, Stanford, California 943052
Hyoungsub Kim
Affiliation:
Department of Material Science and Engineering, Stanford University, Stanford, California 94305
Paul C. McIntyre
Affiliation:
Department of Material Science and Engineering, Stanford University, Stanford, California 94305
Stacey F. Bent
Affiliation:
Department of Chemical Engineering, Stanford University, Stanford, California 94305
Get access

Abstract

A series of self-assembled molecules have been investigated as deactivating agents for the HfO2 atomic layer deposition (ALD). Three important factors of self-assembled monolayers (SAMs) deactivating efficiency towards ALD--chain length, reactivity and steric effect--have been investigated and discussed as well as the initial blocking mechanism of this process. This investigation shows that in order to achieve satisfactory deactivation, it is crucial to choose high reactivity, low steric effect molecules with certain chain length to form condensed, high hydrophobic organic monolayers.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Packan, P., Science 285, 2079 (1999).Google Scholar
2. Wilk, G. D., and Wallace, R. M., Appl. Phys. Lett. 76, 112 (2000).Google Scholar
3. Golzhauser, A., Geyer, W., Stadler, V., Eck, W., Grunze, M., Edinger, K., Weimann, T., and Hinze, P., J. Vac. Sci. Tech. B 18, 3414 (2000).Google Scholar
4. Kang, L., Jeon, Y., Onishi, K., Lee, B. H., Qi, W-J., Nieh, R., Gopalan, S., and Lee, J. C., Technical Digest of VLSI Symposium, P. 44 (2000).Google Scholar
5. Ritala, M., Kukli, K., Rahtu, A., Rälsänen, P. I., Lesklä, M., Sajavaara, T., and Keinonen, J., Science 288, 319 (2000).Google Scholar
6. Chen, R., Kim, H., McIntyre, P. C., and Bent, S. F., Appl. Phys. Lett. accepted.Google Scholar
7. Yanm, M., Koide, Y., Babcock, J. R., Markworth, P. R., Belot, J. A., Marks, T. J., and Chang, R. P. H., Appl. Phys. Lett. 79, 1709 (2001)Google Scholar
8. Chen, R., Mui, C., Musgrave, C. B., Bent, S. F., unpublished date.Google Scholar