Hostname: page-component-68c7f8b79f-fcrnt Total loading time: 0 Render date: 2025-12-23T01:40:59.776Z Has data issue: false hasContentIssue false

Atomistic Simulation of Dislocation Interactions with a σ = 5 (210) Grain Boundary during Nanoindentation of Ni

Published online by Cambridge University Press:  15 March 2011

Ho Jang
Affiliation:
Department of Materials Science and Engineering, Korea University, Seoul, 136-701, Korea
Diana Farkas
Affiliation:
Department of Materials Science and Engineering, Virginia Polytechnic Institute, Blacksburg, VA 24061, USA
Get access

Abstract

Molecular dynamics simulations of nanoindentation were performed using embedded atom potentials. The indentation was simulated on a Ni substrate using a diamond-like spherical indenter. In this study, we focused on the interaction of a σ=5 (210) grain boundary with the dislocations that were nucleated and expanded as loops under the indenter during nano- indentation. The results showed that dislocation loops were nucleated beneath the surface and propagated on multiple {111} slip planes. These dislocations impinged into the grain boundary in the course of nanoindentation. The lattice dislocations changed the atom configuration at the boundary region as they merged into the grain boundary and at later stages they transmitted across the grain boundary. The results also showed that the presence of a grain boundary affected the indenting speed and dislocation motion during nanoindentation, with the grain boundary retarding the indentation process.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

[1] Gane, N. and Bowden, F.P., J. Appl. Phys. 39, 1432 (1968).Google Scholar
[2] Moody, N.R., Gerberich, W.W., Burnham, N., and Baker, S.P. (ed.), Fundamentals of Nanoindentation and Nanotribology, MRS Proc. 522 (1998).Google Scholar
[3] Kramer, D.E., Yoder, K.B., Gerberich, W.W., Phil. Mag. A, 81, 2033 (2001).Google Scholar
[4] Corcoran, S.G., Colton, R.J, Lilleodden, E.T., and Gerberich, W.W., Phy. Rev. B, 55, R16 057 (1997).Google Scholar
[5] Suresh, S., Nieh, T.-G., and Choi, B.W., Scripta Mater. 41, 951 (1999).Google Scholar
[6] Kiely, J.D. and Houston, J.E., Phys. Rev. B, 57, 12 588 (1998).Google Scholar
[7] Figuera, J. de la, Gonzalez, M.A., Garcia-Martinez, R., Rojo, J.M., Herman, O.S., Parga, V.L. Vazquez de, and Miranda, R., Phys. Rev. B, 58, 1169 (1998).Google Scholar
[8] Kelchner, C., Plimpton, S.J., and Hamilton, J.C., Phys. Rev. B, 58, 11 058 (1998).Google Scholar
[9] Gouldstone, A., Vliet, K.J. Van, Suresh, S., Nature, 411, 656 (2001).Google Scholar
[10] Zimmerman, J.A., Kelchner, C.L., Klein, P.A., Hamilton, J.C., and Foiles, S.M., Phys. Rev. Lett., 87, 165507 (2001).Google Scholar
[11] Li, J., Vliet, K.J. Van, Zhu, T., Yip, S, and Suresh, S., Nature, 418, 307 (2002).Google Scholar
[12] Feichtinger, D., Derlet, P.M., and Swygenhoven, H. Van, Phys. Rev. B 67, 024113 (2003).Google Scholar
[13] Voter, A.F. and Chen, S.P., Mat. Res. Soc. Symp. 82. 175 (1987).Google Scholar
[14] Swygenhoven, H. Van, Spaczer, M., and Caro, A., Acta mater. 47, 10, 317 (1999).Google Scholar
[15] swygnhoven, H. Van, Derlet, P.M., and Hasnaoui, A, Phys. Rev. B, 66 024101 (2002).Google Scholar
[16] Petch, N.J., Iron, J. and Steel Institute, 174, 25 (1953).Google Scholar
[17] Grimmer, H., Bollmann, W. and Warringron, D.H., Acta Crystall. A 30, 197 (1974).Google Scholar
[18] Balluffi, R.W., Brokman, A., and King, A. H., Acta Metall. 30, 1453 (1982).Google Scholar