Anisotropy of Nanoindentation – a tool for the determination of nanocrystal orientation ?

Published online by Cambridge University Press:  15 February 2011

David Christopher
Affiliation:
Mathematical, Sciences, Loughborough University, Loughborough, Leicestershire, LE11 3TU, UK.
Steven Kenny
Affiliation:
Mathematical, Sciences, Loughborough University, Loughborough, Leicestershire, LE11 3TU, UK.
Roger Smith
Affiliation:
Mathematical, Sciences, Loughborough University, Loughborough, Leicestershire, LE11 3TU, UK.
Asta Richter
Affiliation:
Engineering Physics, University of Applied Sciences, Wildau, Bahnhofstrasse, 15745 Wildau, Germany.
Bodo Wolf
Affiliation:
Engineering Physics, University of Applied Sciences, Wildau, Bahnhofstrasse, 15745 Wildau, Germany.
Bruce King
Affiliation:
Physics Department, University of Newcastle, Callaghan, NSW 2308, Australia.
Get access

Abstract

The pile up patterns arising in nanoindentation are shown to be indicative of the sample crystal symmetry. To explain and interpret these patterns, complementary molecular dynamics simulations and experiments have been performed to determine the atomistic mechanisms of the nanoindentation process in single crystal Fe{110}. The simulations show that dislocation loops start from the tip and end on the crystal surface propagating outwards along the four in-plane <111> directions. These loops carry material away from the indenter and form bumps on the surface along these directions separated from the piled-up material around the indenter hole. Atoms also move in the two out-of-plane <111> directions causing propagation of subsurface defects and pile-up around the hole. This finding is confirmed by scanning force microscopy mapping of the imprint, the piling-up pattern proving a suitable indicator of the surface crystallography. Experimental force-depth curves over the depth range of a few nanometers do not appear smooth and show distinct pop-ins. On the sub-nanometer scale these pop-ins are also visible in the simulation curves and occur as a result of the initiation of the dislocation loops from the tip.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Olivier, W.C. and Pharr, G.M. J. Mater. Res. 7 1562 (1992)Google Scholar
2. Landmann, U., Luedtke, W.D., Burnham, N. A. and Colton, R.J., Science 248, 454 (1990).Google Scholar
3. Kelchner, C.L., Plimpton, S.J., Hamilton, J.C. Phys. Rev. B 58, 11085 (1998).Google Scholar
4. Kiely, J.D. and Houston, J.E. Phys. Rev. B 57, 12588 (1998).Google Scholar
5. Corcoran, S.G., Colton, R.J., Lilleodden, E.T. and Gerberich, W.W. Phys. Rev. B 55, R16057 (1997).Google Scholar
6. Fuente, O. Rodriguez de la, Zimmerman, J.A., Gonzalez, M.A., Figuera, J. de la, Hamilton, J.C., Pai, W. W. and Rojo, J.M., Phys. Rev. Lett. 88, 036101 (2002).Google Scholar
7. Perez, R., Payne, M.C. and Simpson, A.D. Phys. Rev. Lett. 75, 4748 (1995).Google Scholar
8. Astala, R., Niemenen, R.M. and Heine, T. Phys. Rev. B 61, 2973 (2000).Google Scholar
9. Richter, A., Ries, R., Smith, R., Henkel, M. and Wolf, B. Diamond Rel. Mater. 9 170 (2000)Google Scholar
10. Christopher, D., Richter, A. and Smith, R. Nanotechnology 12 372 (2001).Google Scholar
11. Ackland, G.J.,Tichy, G., Vitek, V. andFinnis, M.W. Philos. Mag. A 50 145 (1987).Google Scholar
12. Brenner, D. W. Phys. Rev. B 42, 9458 (1990). Phys. Rev. B 46, 1948 (1992).Google Scholar
13. Lindhard, J. and Scharff, M. Phys. Rev. 124 128 (1961).Google Scholar
14. Ziegler, J.F., Biersack, J.P. and Littmark, U. The Stopping and Range of Ions in Solids, (Pergamon Press, Oxford, 1985)Google Scholar
15. Smith, R., Christopher, D., Kenny, S.D., Richter, A. and Wolf, B. Phys. Rev. B (2003) in press.Google Scholar