An in-situ TEM Nanoindenter System with 3-axis Inertial Positioner

Published online by Cambridge University Press:  10 February 2011

M.S. Bobji
Affiliation:
Department of Materials, University of Oxford, Oxford, OX1 3PH, U.K.
C.S. Ramanujan
Affiliation:
Department of Materials, University of Oxford, Oxford, OX1 3PH, U.K.
R.C. Doole
Affiliation:
Department of Materials, University of Oxford, Oxford, OX1 3PH, U.K.
J.B. Pethica
Affiliation:
Department of Materials, University of Oxford, Oxford, OX1 3PH, U.K.
B.J. Inkson
Affiliation:
Dept. of Engineering Materials, University of Sheffield, Sheffield, S1 3JD, U.K.
Get access

Abstract

To quantify the mechanical properties and deformation behaviour of sub-micron wires, an in-situ nanoindenter system is being developed for a TEM. The miniaturized displacement controlled nanoindenter fits inside a side entry specimen holder. For coarse positioning, a novel 3-axis inertial positioner has been developed. This positioner has a range of 5mm with a 300 nm resolution. The fine displacements are generated by means of a tube piezo and the force is measured using a fibre optic interferometer.

Type
Research Article
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Siegel, R.W. and Fougere, G.E., Nanostructured materials, 6, 205 (1995).Google Scholar
2. Savader, J.B., Scanlon, M.R., Cammarata, R.C., Smith, D.T. and Hayzelden, C., Scripta Mater., 36 (1), 29 (1997).Google Scholar
3. Josell, D., Heerden, D. van, Read, D., Bonevich, J. and Shechtman, D., J. Mater. Res., 13, 10 (1998).Google Scholar
4. Mitchell, T.E., Lu, Y.C., Griffin, A.J., Natasi, M. and Kung, H., J. Am. Ceram. Soc., 80 (7), 1673 (1997)Google Scholar
5. Clemens, B.M., Kung, H. and Barnett, S.A., MRS Bulletin, 24 (2), 20 (1999).Google Scholar
6. Sproul, W.D., Science, 273, 889 (1996).Google Scholar
7. Pethica, J. B., Hutchings, R., and Oliver, W.C., Phil. Mag. A, 48 (4), 593 (1983),.Google Scholar
8. Kizuka, T., Yamada, K., Deguchi, S., Naruse, M. and Tanaka, N., Phy. Rev B 55 R7398 (1997).Google Scholar
9. Wall, M.A. and Dahmen, U., Microsc. Res. & Tech. 42, 248 (1998).Google Scholar
10. Pohl, D.W. (1987) Surf. Sci. 181, 174.Google Scholar