Hostname: page-component-857557d7f7-zv5th Total loading time: 0 Render date: 2025-11-22T06:39:41.341Z Has data issue: false hasContentIssue false

Reaction kinetics of Cu2-xS, ZnS, and SnS2 to form Cu2ZnSnS4 and Cu2SnS3 studied using differential scanning calorimetry

Published online by Cambridge University Press:  30 May 2017

Elizabeth A. Pogue*
Affiliation:
University of Illinois Urbana-Champaign, Department of Materials Science and Engineering, Champaign, IL 61801, U.S.A.
Melissa Goetter
Affiliation:
University of Illinois Urbana-Champaign, Department of Materials Science and Engineering, Champaign, IL 61801, U.S.A.
Angus Rockett
Affiliation:
University of Illinois Urbana-Champaign, Department of Materials Science and Engineering, Champaign, IL 61801, U.S.A. Colorado School of Mines, Department of Metallurgical and Materials Engineering, Golden, CO 80401, U.S.A.
*

Abstract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Differential scanning calorimetry experiments on mixed Cu2-xS, ZnS, and SnS2 precursors were conducted to better understand how Cu2ZnSnS4 (CZTS) and Cu2SnS3 form. The onset temperatures of Cu2SnS3 reactions and CZTS suggest that the ZnS phase may mediate Cu2SnS3 formation at lower temperatures before a final CZTS phase forms. We also found no evidence of a stable Cu2ZnSn3S8 phase. The major diffraction peaks associated with Cu2ZnSnS4, and Cu2SnS3 (overlaps with ZnS, as well) began to grow around 380 °C, although the final reaction to form Cu2ZnSnS4 probably did not occur until higher temperatures were reached. An exothermic reaction was observed corresponding to formation of this phase. There was some variability in the onset temperature for reactions to form Cu2SnS3. At least 5 steps are involved in this reaction and several segments of the reaction had relatively reproducible energies.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2017 

References

REFERENCES

Wang, W., Winkler, M.T., Gunawan, O., Gokmen, T., Todorov, T.K., Zhu, Y., and Mitzi, D.B., Adv. Energy Mater. 4, 1301465 (2014).Google Scholar
Maeda, T., Nakamura, S., and Wada, T., Jpn. J. Appl. Phys. 50, 04DP07 (2011).CrossRefGoogle Scholar
Schurr, R., Hölzing, A., Jost, S., Hock, R., Voβ, T., Schulze, J., Kirbs, A., Ennaoui, A., Lux-Steiner, M., Weber, A., Kötschau, I., and Schock, H.-W., Thin Solid Films 517, 2465 (2009).CrossRefGoogle Scholar
Fairbrother, A., Fontané, X., Izquierdo-Roca, V., Espíndola-Rodríguez, M., López-Marino, S., Placidi, M., Calvo-Barrio, L., Pérez-Rodríguez, A., and Saucedo, E., Sol. Energy Mater. Sol. Cells 112, 97 (2013).Google Scholar
Weber, A., Mainz, R., Unold, T., Schorr, S., and Schock, H.-W., Phys. Status Solidi 6, 1245 (2009).Google Scholar
Schorr, S., Weber, A., Honkimäki, V., and Schock, H.W., Thin Solid Films 517, 2461 (2009).Google Scholar
Baryshev, S. V. and Thimsen, E., Chem. Mater. 27, 2294 (2015).CrossRefGoogle Scholar
Kubaschewski, O., Alcock, C.B., and Spencer, P.J., Materials Thermochemistry, 6th ed. (Pergamon Press, New York, 1993) pp. 258323.Google Scholar
Buerger, M.J. and Wuensch, B.J., Science (80-. ). 141, 276 (1963).CrossRefGoogle Scholar
Valakh, M.Y., Dzhagan, V.M., Babichuk, I.S., Fontane, X., Perez-Rodriquez, A., and Schorr, S., JETP Lett. 98, 255 (2013).Google Scholar
Dimitrievska, M., Fairbrother, A., Pérez-Rodríguez, A., Saucedo, E., and Izquierdo-Roca, V., Acta Mater. 70, 272 (2014).Google Scholar
Paris, M., Choubrac, L., Lafond, A., Guillot-Deudon, C., and Jobic, S., Inorg. Chem. 53, 8646 (2014).Google Scholar