Giant dielectric constant in Al2O3/TiO2 multilayer films synthesized by atomic layer deposition

Published online by Cambridge University Press:  22 January 2018

Takuji Tsujita*
Affiliation:
Advanced Research Division, Panasonic Corporation, Kadoma, Osaka, Japan Panasonic Science Research Alliance Laboratory, Graduate School of Engineering, Osaka University, Suita, Osaka, Japan
Yukihiro Morita
Affiliation:
Advanced Research Division, Panasonic Corporation, Kadoma, Osaka, Japan Panasonic Science Research Alliance Laboratory, Graduate School of Engineering, Osaka University, Suita, Osaka, Japan
Mikihiko Nishitani
Affiliation:
Panasonic Science Research Alliance Laboratory, Graduate School of Engineering, Osaka University, Suita, Osaka, Japan
Get access

Abstract

Multilayer films formed from Al2O3 and TiO2 by atomic layer deposition were systematically studied. The relationship between the electrical characteristics of the films and the type of oxidizer used for the Al2O3 layers was investigated. The results indicated that oxygen defects in TiO2 layer and a highly insulating Al2O3 layer are necessary for realizing a giant dielectric constant and a low dielectric loss. A high electrical resistance of 1.7×108 Ω / diameter of 1 mm and a dielectric constant of 1140 were achieved at 100 Hz by suitable choice of oxidizer for the Al2O3 layer.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2018 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Mikhelashvili, V., Garshtein, E. and Eisenstein, G., IEEE Electron Device Lett. 27(5), 344 (2006).CrossRefGoogle Scholar
Auciello, O., Fan, W., Kabius, B., Saha, S. and Carisle, J. A., Chang, R. P. H., Lopez, C., Irena, E. E. and Baragiola, R. A., Appl. Phys. Lett. 86, 042904 (2005).CrossRefGoogle Scholar
Kim, S. K., Choi, G. J., KIM, J. H. and Hwang, C. S., Chem. Mater. 20, 3723 (2008).CrossRefGoogle Scholar
Li, W., Auciello, O., Premnath, R. N. and Kabius, B., Appl. Phys. Lett. 96, 162907 (2010).CrossRefGoogle Scholar
Lee, G., Lai, B., Phatak, C., Katiyar, R. S. and Auciello, O., J. Appl. Phys. 114, 027001 (2013).CrossRefGoogle Scholar