Hostname: page-component-68c7f8b79f-lqrcg Total loading time: 0 Render date: 2025-12-20T15:39:57.207Z Has data issue: false hasContentIssue false

Fabrication of Nitride Thin Films on Si Substrates by Atomic Layer Deposition Technique

Published online by Cambridge University Press:  26 February 2018

Shumpei Ogawa
Affiliation:
Department of Electronic and Engineering, Graduate School of Engineering, Saitama Institute of Technology
Tatsuya Kuroda
Affiliation:
Department of Information Systems, Faculty of Engineering, Saitama Institute of Technology
Ryuga Koike
Affiliation:
Department of Information Systems, Faculty of Engineering, Saitama Institute of Technology
Hiroki Ishizaki*
Affiliation:
Department of Electronic and Engineering, Graduate School of Engineering, Saitama Institute of Technology Department of Information Systems, Faculty of Engineering, Saitama Institute of Technology
*
Get access

Abstract

Recently, Plasma Assisted Atomic Layer Deposition Technique will easily control the thickness and the composition of semiconductor films. The radical generated by using the plasma techniques, gave the decrease of the defect into the semiconductor films. In this investigation, the relationship between microwave plasma power, nitrogen gas flow rate and concentration of generated nitrogen radical, was evaluated. At the first, Plasma emission spectrum at microwave plasma power (0 to 400W) was measured using a mixed 200sccm argon gas and 10sccm nitrogen gas. Next, the plasma emission spectrum was measured in the mixing of nitrogen gas flow rate (0 to 40sccm) with 200sccm argon gas flow rate. At that time, the microwave plasma power was set to 200W. Nitrogen radical spectrum were identified from all the emission spectrum, and the nitrogen radical intensity was calculated. As a result, the nitrogen radical intensity became the largest at 200sccm argon gas flow rate and 10sccm nitrogen gas flow rate. In addition, the nitrogen radical intensity increased in proportion to the microwave plasma power. The concentration of generated nitrogen radical could be controlled by changing the microwave plasma power and the nitrogen gas flow rate. Mentioned above, nitride thin films will be obtained on Si Substrates by microwave generated remote plasma assisted atomic layer deposition technique.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2018 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

References:

Chen, M. J., Shin, Y. T., Wu, M. K. and Tsai, F. Y., J. Appl. Phys., 101, 033130 (2007).Google Scholar
Gusev, E. P., Copel, M., Chartier, E., Baumvol, I. J. R., Krug, C., and Gribelyuk, M. A., Appl. Phys. Lett.,76, 176 (2000).Google Scholar
Toyoda, S., Okabayashi, J., Kumigashira, H., Oshima, M., Ono, K., Niwa, M., Usuda, K. and Liu, G.L., Appl. Phys. Lett, 84, 2328 (2004).CrossRefGoogle Scholar
Xuan, Y., Ye, P. D., Lin, H. C. and Wilk, G. D., Appl. Phys. Lett., 89, 132103 (2006).CrossRefGoogle Scholar