Synchrotron scattering and nanoindentation of heat treated high performance thermotropic polymer

Published online by Cambridge University Press:  12 November 2018

A. Romo-Uribe*
Affiliation:
Polymer Nanocomposites Laboratory LNyC, Cuernavaca Mor.62230, MEXICO
A. Reyes-Mayer
Affiliation:
Centro de Caracterización e Investigación en Materiales S.A. de C. V., Calle 21 Este #205, Bodega F, Col. Civac, Jiutepec, Mor.62578, MEXICO Universidad Tecnologica Emiliano Zapata del Estado de Morelos UTEZ, Av. Universidad Tecnologica No. 1, Col. Palo Escrito, Emiliano Zapata, Mor.62760, MEXICO
E. Sarmiento-Bustos
Affiliation:
Universidad Tecnologica Emiliano Zapata del Estado de Morelos UTEZ, Av. Universidad Tecnologica No. 1, Col. Palo Escrito, Emiliano Zapata, Mor.62760, MEXICO
M. Calixto-Rodriguez
Affiliation:
Universidad Tecnologica Emiliano Zapata del Estado de Morelos UTEZ, Av. Universidad Tecnologica No. 1, Col. Palo Escrito, Emiliano Zapata, Mor.62760, MEXICO
K. Santiago-Santiago
Affiliation:
Universidad Tecnologica Emiliano Zapata del Estado de Morelos UTEZ, Av. Universidad Tecnologica No. 1, Col. Palo Escrito, Emiliano Zapata, Mor.62760, MEXICO
Get access

Abstract

A multi-scale analysis, ranging from μm → nm → Å-scaie on the influence of thermal treatment on the thermotropic copolyester based on 60 mol% (l,4)-hydroxybenzoic acid (B), 5 mol% (2,6)-hydroxynaphthoic acid (N), 17.5 mol% terephthalic acid (T) and 17.5 mol% biphenol (BP) - COTBP- was carried out. The Å and nm-scale structure was investigated by synchrotron scattering (WAXS and SAXS). Extruded tapes ca. 30 μm thick were annealed at 300 °C under air, without tension. WAXS revealed fibre-like structure with crystalline order, whereas SAXS patterns exhibited diamond-shaped diffuse scattering and discrete meridional scattering elucidating structures along the fibre axis and periodic crystallites. Heat treatment produced roughness reduction, and WAXS patterns showed reflections sharpening indicating an improvement of molecular register and packing (molecular alignment and degree of crystallinity Χ increased). Thermal treatment increased the thermal stability, melting transition and tensile Young’s modulus, E, along extrusion axis, whereas nanoindentation showed decrease of hardness and elastic modulus. Hence, a thermally-induced seif-reinforcing effect was evidenced, with microstructure reorganization correlating with improved thermo-mechanical properties.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2018 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

Calundann, G. W., Jaffe, M., Anisotropic polymers, their synthesis and properties. Proc Robert A. Welch Con f. Chetm. Res. XXVI. Syn. Polymers 2, 247-285 (1982).Google Scholar
Donald, A. M., Windle, A. H., Hanna, S., Liquid Crystalline Polymers, 2nd edition, Cambridge University Press, United Kingdom (2005).Google Scholar
Salahshoor-Kordestani, S., Hanna, S., Windle, A. H., Polymer 4, 6619-26 (2000).CrossRefGoogle Scholar
Reyes-Mayer, A., Alvarado-Tenorio, B., Romo-Uribe, A., Jaffe, M., Polym. Adv. Techn. 24, 1029-1039 (2013).CrossRefGoogle Scholar
Ran, S., Fang, D., Zong, X., Hsiao, B. S., Chu, B., Cunniff, P. M., Polymer 42, 1601-1612 (2001).CrossRefGoogle Scholar
Reyes-Mayer, A., Alvarado-Tenorio, B., Romo-Uribe, A., Benavente, R., Jaffe, M., Molina-Ocampo, A., Polym. Adv. Techn. 27, 748-758 (2016).CrossRefGoogle Scholar
Romo-Uribe, A., Reyes-Mayer, A., Calixto-Rodriguez, M, Benavente, R., Jaffe, M., Polymer 153, 408-421 (2018).CrossRefGoogle Scholar
Yoffe, E. H., Phil. Mag. A 50, 813-828 (1984).CrossRefGoogle Scholar