Surface analysis of the selective oxidation during austeniticannealing of CMnSi high strength steel

Published online by Cambridge University Press:  10 April 2009

Get access

Abstract

The selective oxidation of three CMnSi steels with differentC levels was studied by XPS. The formation of a graduallycovering SiO2 film is observed until a transition temperatureabove which the oxide film disappears, resulting in a renewedappearance of metallic iron at the surface. This change inoxidation behavior is thought to be due to the SiO2 reductionby solute C which is thermodynamically favorable at hightemperature. At the same time the precipitation of a BN filmon the metallic surface was observed which prevented anyfurther oxidation.

Information

Type
Research Article
Copyright
© La Revue de Métallurgie, 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable