Metallurgical quality characterization of nickel-basedsuperalloys

Published online by Cambridge University Press:  22 May 2007

Get access

Abstract

A new image analyzer, Thixomet®, has been developed with the abilityto create “panoramic” images of material microstructure forinvestigations. Capabilities of the Thixomet image analyzer for materialmicrostructural characterization are demonstrated with examplesof nickel-based superalloys. Practical use of the Thixomet forcontrolling material properties by characterizing their microstructureis demonstrated.

Information

Type
Research Article
Copyright
© La Revue de Métallurgie, 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable