Strain rate dependence of plastic flow in Ce-based bulk metallic glass during nanoindentation

Published online by Cambridge University Press:  03 March 2011

B.C. Wei*
Affiliation:
National Microgravity Laboratory, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, People’s Republic of China
L.C. Zhang
Affiliation:
National Microgravity Laboratory, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, People’s Republic of China
T.H. Zhang
Affiliation:
State Key Laboratory of Nonlinear Mechanics (LNM), Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, People’s Republic of China
D.M. Xing
Affiliation:
State Key Laboratory of Nonlinear Mechanics (LNM), Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, People’s Republic of China
J. Das
Affiliation:
FG Physikalische Metallkunde, FB 11 Material- und Geowissenschaften, Technische Universität Darmstadt, D-64287 Darmstadt, Germany; and Leibniz-Institut für Festkörperund Werkstoffforschung Dresden, Helmholtzstrasse 20, D-01069 Dresden, Germany
J. Eckert
Affiliation:
FG Physikalische Metallkunde, FB 11 Material- und Geowissenschaften, Technische Universität Darmstadt, D-64287 Darmstadt, Germany; and Leibniz-Institut für Festkörperund Werkstoffforschung Dresden, Helmholtzstrasse 20, D-01069 Dresden, Germany
*
a)Address all correspondence to this author. e-mail: weibc@imech.ac.cn
Get access

Abstract

The strain rate dependence of plastic deformation of Ce60Al15Cu10Ni15 bulk metallic glass was studied by nanoindentation. Even though the ratio of room temperature to the glass transition temperature was very high (0.72) for this alloy, the plastic deformation was dominated by shear banding under nanoindentation. The alloy exhibited a critical loading rate dependent serrated flow feature. That is, with increasing loading rate, the alloy exhibited a transition from less prominent serrated flow to pronounced serrated flow during continuous loading but from serrated to smoother flow during stepped loading.

Information

Type
Reviews
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1Spaepen, F.: A microscopic mechanism for steady state inhomogeneous flow in metallic glasses. Acta Metall. 25, 407 (1977).Google Scholar
2Argon, A.S.: Plastic deformation in metallic glasses. Acta Metall. 27, 47 (1979).CrossRefGoogle Scholar
3Kawamura, Y. and Inoue, A.: Newtonian viscosity of supercooled liquid in a Pd40Ni40P20 metallic glass. Appl. Phys. Lett. 77, 1114 (2000).CrossRefGoogle Scholar
4Chen, H.S., Kato, H., Inoue, A., Saida, J., and Nishiyama, N.: Thermal evidence of stress-induced structural disorder of a Zr55Al10Ni5Cu30 glassy alloy in the non-Newtonian region. Appl. Phys. Lett. 79, 60 (2001).Google Scholar
5Nieh, T.G., Wadsworth, J., Liu, C.T., Ohkubo, T., and Hirotsu, Y.: Plasticity and structural instability in a bulk metallic glass deformed in the supercooled liquid region. Acta Mater. 49, 2887 (2001).CrossRefGoogle Scholar
6Demetriou, M.D. and Johnson, W.L.: Modeling the transient flow of undercooled glass-forming liquids. J. Appl. Phys. 95, 2857 (2004).CrossRefGoogle Scholar
7Reger-Leonhard, A., Xing, L.Q., Heilmaier, M., Gebert, A., Eckert, J., and Schultz, L.: Effect of crystalline precipitations on the mechanical behavior of bulk glass forming Zr-based alloys. Nanostruct. Mater. 10, 805 (1998).CrossRefGoogle Scholar
8Reger-Leonhard, A., Heilmaier, M., and Eckert, J.: Newtonian flow of Zr55Cu30Al10Ni5 bulk metallic glassy alloys. Scripta Mater. 43, 459 (2000).Google Scholar
9Chen, H.S.: Plastic flow in metallic glasses under compression. Scripta Metall. 7, 931 (1973).CrossRefGoogle Scholar
10Wright, W.J., Saha, R., and Nix, W.D.: Deformation mechanisms of the Zr40Ti14Ni10Cu12Be24 bulk metallic glass. Mater. Trans. 42, 642 (2001).CrossRefGoogle Scholar
11Schuh, C.A. and Nieh, T.G.: A survey of instrumented indentation studies on metallic glasses. J. Mater. Res. 19, 46 (2004).Google Scholar
12Schuh, C.A., Lund, A.C., and Nieh, T.G.: New regime homogeneous flow in the deformation map of metallic glasses: Elevated temperature nanoindentation experiments and mechanistic modeling. Acta Mater. 52, 5879 (2004).Google Scholar
13Zhang, G.P., Wang, W., Zhang, B., Tan, J., and Liu, C.S.: On rate-dependent serrated flow behavior in amorphous metals during nanoindentation. Scripta Mater. 52, 1147 (2005).CrossRefGoogle Scholar
14Greer, A.L., Castellero, A., Madge, S.V., Walker, I.T., and Wilde, J.R.: Nanoindentation studies of shear banding in fully amorphous and partially devitrified metallic alloys. Mater. Sci. Eng., A 375–377, 1182 (2004).CrossRefGoogle Scholar
15Jiang, W.H., Pinkerton, F.E., and Atzmon, M.: Mechanical behavior of shear bands and the effect of their relaxation in a rolled amorphous Al-based alloy. Acta Mater. 53, 3469 (2005).CrossRefGoogle Scholar
16Wei, B.C., Zhang, T.H., Li, W.H., Sun, Y.F., Yu, Y., and Wang, Y.R.: Serrated plastic flow during nanoindentation in Nd-based bulk metallic glasses. Intermetallics 12, 1239 (2004).CrossRefGoogle Scholar
17Li, W.H., Zhang, T.H., Xing, D.M., Wei, B.C., Wang, Y.R., and Dong, Y.D.: Instrumented indentation study of plastic deformation in bulk metallic glasses. J. Mater. Res. 21, 75 (2006).Google Scholar
18Concustell, A., Sort, J., Alcala, G., Mato, S., Gebert, A., Eckert, J., and Baro, M.D.: Plastic deformation and mechanical softening of Pd40Cu30Ni10P20 bulk metallic glass during nanoindentation. J. Mater. Res. 20, 2719 (2005).CrossRefGoogle Scholar
19Wei, B.C., Zhang, T.H., Li, W.H., Xing, D.M., Zhang, L.C., and Wang, Y.R.: Indentation creep behavior in Ce-based bulk metallic glasses at room temperature. Mater. Trans. 46, 2959 (2005).CrossRefGoogle Scholar
20Ramamurty, U., Jana, S., Kawamura, Y., and Chattopadhyay, K.: Hardness and plastic deformation in a bulk metallic glass. Acta Mater. 53, 705 (2005).CrossRefGoogle Scholar
21Wei, B.C., Zhang, T.H., Zhang, L.C., Xing, D.M., Li, W.H., and Liu, Y.: Plastic deformation in Ce-based bulk metallic glasses during depth-sensing indentation. Mater. Sci. Eng., A 2006, doi: 10.1016/j.msea.2006.01.161.Google Scholar
22Poisl, W.H., Oliver, W.C., and Fabes, B.D.: The relationship between indentation and uniaxial creep in amorphous selenium. J. Mater. Res. 10, 2024 (1995).Google Scholar
23Yang, A., Riester, L., and Nieh, T.G.: Strain hardening and recovery in a bulk metallic glass under nanoindentation. Scripta Mater. 54, 1277 (2006).Google Scholar
24Falk, M.L. and Langer, J.S.: Dynamics of viscoplastic deformation in amorphous solids. Phys. Rev. E 57, 7192 (1998).Google Scholar
25Russew, K., Hey, P.D., Sietsma, J., and Beukel, A.V.D.: Viscous flow of amorphous Fe40Ni40Si6B14 studied by direct creep measurements and relaxation of bend stresses under nonisothermal conditions. Acta Mater. 45, 2129 (1997).Google Scholar