Residual stresses in DLC/Si and Au/Si systems: Application of a stress-relaxation model to the nanoindentation technique

Published online by Cambridge University Press:  31 January 2011

Yun-Hee Lee
Affiliation:
School of Materials Science and Engineering, Seoul National University, Seoul 151–742, Korea
Dongil Kwon*
Affiliation:
School of Materials Science and Engineering, Seoul National University, Seoul 151–742, Korea
*
a)Address all correspondence to this author.donglik@gong.snu.ac.kr
Get access

Abstract

Residual stress in a thin film was analyzed by the nanoindentation technique. Two dominant effects of residual stress to indentation were summarized as the slope change in loading curve and the invariant value of intrinsic hardness. A stress-sensitive reversibly deformed zone around contact was modeled to explain the indentation behaviors under a residually stressed state. Finally, the residual stress was evaluated from the changes in contact shape and applied load during stress relaxation under the condition of constant indentation depth. The residual stresses in diamond-like carbon and Au films analyzed from this model agreed well with the average values measured by the curvature method.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1Noyan, I.C. and Cohen, J.B., Residual Stresses (Springer-Verlag, New York, 1987).CrossRefGoogle Scholar
2Eberhardt, A.W., Pandey, R., Williams, J.M., Weimer, J.J., Ila, D., and Zimmerman, R.L., Mater. Sci. Eng. A 229, 147 (1997).CrossRefGoogle Scholar
3Karlsson, L., Hultman, L., and Sundgren, J.E., Thin Solid Films 371, 167 (2000).CrossRefGoogle Scholar
4Uhlmann, E. and Klein, K., Surf. Coat. Technol. 131, 448 (2000).CrossRefGoogle Scholar
5Fang, W. and Lo, C-Y., Sens. Actuators 84, 310 (2000).CrossRefGoogle Scholar
6Ruud, C.O., DiMascio, P.S., and Yavelak, J.J., Exp. Mech. 25, 338 (1985).CrossRefGoogle Scholar
7Perry, A.J., Sue, J.A., and Martin, P.J., Surf. Coat. Technol. 81, 17 (1996).CrossRefGoogle Scholar
8Bergman, L. and Nemanich, R.J., J. Appl. Phys. 78, 6709 (1995).CrossRefGoogle Scholar
9Flinn, P.A., in Thin Films: Stresses and Mechanical Properties Proc. 130, edited by Brauman, J.C., Nix, W.D., Barnett, D.M., and Smith, D.A. (Mater. Res. Soc. Symp. Proc. 130, Pittsburgh, PA, 1989), p. 41.Google Scholar
10Doerner, M.F. and Nix, W.D., J. Mater. Res. 1, 601 (1986).CrossRefGoogle Scholar
11Pharr, G.M. and Oliver, W.C., MRS Bull. July, 28 (1992).CrossRefGoogle Scholar
12Sines, G. and Carlson, R., ASTM Bull. February, 35 (1952).Google Scholar
13Underwood, J.H., Exp. Mech. 13, 373 (1973).CrossRefGoogle Scholar
14LaFontaine, W.R., Paszkiet, C.A., Korhonen, M.A., and Li, C-Y., J. Mater. Res. 6, 2084 (1991).CrossRefGoogle Scholar
15Tsui, T.Y., Oliver, W.C., and Pharr, G.M., J. Mater. Res. 11, 752 (1996).CrossRefGoogle Scholar
16Bolshakov, A., Oliver, W.C., and Pharr, G.M., J. Mater. Res. 11,760 (1996).CrossRefGoogle Scholar
17Suresh, S. and Giannakopoulos, A.E., Acta Mater. 46, 5755 (1998).CrossRefGoogle Scholar
18Tsui, T.Y. and Pharr, G.M., J. Mater. Res. 14, 292 (1999).CrossRefGoogle Scholar