Prediction of nanoindentation hardness profile from a load-displacement curve

Published online by Cambridge University Press:  31 January 2011

K. W. Xu
Affiliation:
State Key Laboratory for Mechanical Behavior of Materials, Xian Jiaotong University, China
G. L. Hou
Affiliation:
State Key Laboratory for Mechanical Behavior of Materials, Xian Jiaotong University, China
B. C. Hendrix
Affiliation:
State Key Laboratory for Mechanical Behavior of Materials, Xian Jiaotong University, China
J. W. He
Affiliation:
State Key Laboratory for Mechanical Behavior of Materials, Xian Jiaotong University, China
Y. Sun
Affiliation:
School of Metallurgy and Materials, The University of Birmingham, Birmingham, United Kingdom
S. Zheng
Affiliation:
School of Metallurgy and Materials, The University of Birmingham, Birmingham, United Kingdom
A. Bloyce
Affiliation:
School of Metallurgy and Materials, The University of Birmingham, Birmingham, United Kingdom
T. Bell
Affiliation:
School of Metallurgy and Materials, The University of Birmingham, Birmingham, United Kingdom
Get access

Abstract

During the nanoindentation process, the load and depth data are continuously recorded. A single load-displacement curve is thus expected to contain material property information from the whole depth range indented. In the present paper, a new method to obtain the hardness-depth curve has been derived for small depths from the load-displacement curve measured at a large depth, based on the assumption that the elastic properties of the indented material can be obtained from the indentation depth. Using this method, hardness values can be computed for various small depths from a single load-displacement curve. From a series of nanoindentation experiments, it has been proven that the method can be used on both homogeneous and surface-modified materials, such as fused silica, single crystal tungsten, and plasma nitrided steel with and without an iron nitride Fe4N compound layer. Testings on a series of Ni–P films coated on 15 MnB steel also gave fairly good results.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1.Oliver, W. C., McHargue, C. J., and Zinkle, S. J., Thin Solid Films 153, 185 (1987).CrossRefGoogle Scholar
2.Doerner, M. F. and Nix, W. D., J. Mater. Res. 1, 601 (1986).Google Scholar
3.Atkins, A. G., Met. Sci. 16, 127 (1982).Google Scholar
4.Sakai, M., Metall. Mater. 41, 1751 (1993).CrossRefGoogle Scholar
5.Fleck, N. A., Muller, C. W., Ashby, M. F., and Hutchinson, J. W., Acta Metall. Mater. 42, 475 (1994).CrossRefGoogle Scholar
6.Loubet, J. L., Georges, J. M., Marchesini, O., and Meille, G., J. Tribology 106, 43 (1984).Google Scholar
7.Oliver, W. C. and Pharr, G. M., J. Mater. Res. 7, 1564 (1992).CrossRefGoogle Scholar
8.Bhttacharya, A. K. and Nix, W. D., Int. J. Solids Structures 24, 1297 (1988).Google Scholar
9.King, R. B., Int. J. Solids Structures 23, 1657 (1987).Google Scholar
10.Gao, H. J., Chiu, C. H., and Lee, J. J., Int. J. Solids Structures 29, 2471 (1992).Google Scholar
11.Zheng, S., Ph.D. Thesis, University of Birmingham (1996).Google Scholar
12.Zheng, S., Sun, Y., Bloyce, A., and Bell, T., Mater. Manufacturing Processes 10, 815 (1995).CrossRefGoogle Scholar