Hostname: page-component-68c7f8b79f-fnvtc Total loading time: 0 Render date: 2025-12-23T13:10:59.165Z Has data issue: false hasContentIssue false

Nanoindentation measurement of hardness and modulus anisotropy in Ni3Al single crystals

Published online by Cambridge University Press:  31 January 2011

W. Wang
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, People's Republic of China
K. Lu
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, People's Republic of China
Get access

Abstract

Hardness and elastic modulus of (111), (110), and (001) oriented Ni3Al single crystals were determined by nanoindenter measurements. Obvious elastic modulus anisotropy and hardness anisotropy were observed. The modulus for (001) was about 17% smaller than that for (111), (110). The hardness was found to be strongly dependent on the indentation size and exhibited a small anisotropy at low indentation loads. When the indentation load was increased further, the hardness anisotropy became apparent. The hardness for (111) was observed to be higher compared to (001). The indentation hardness size effect was examined by using strain gradient plasticity theory.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Pharr, G.M. and Oliver, W.C., J. Mater. Res. 7, 1564 (1992).Google Scholar
2.Bahar, D.F., Hoehn, J.W., Moody, N.R., and Gerberich, W.W., Acta Materiala 45, 5163 (1997).CrossRefGoogle Scholar
3.Kieley, J.D. and Houston, J.E., Phys. Rev. B 57, 12588 (1998).CrossRefGoogle Scholar
4.Nix, W.D., Mater. Sci. Eng. A234–236, 37 (1997).CrossRefGoogle Scholar
5.Norwak, R. and Sakai, M., Acta Metall. Mater. 42, 2879 (1994).CrossRefGoogle Scholar
6.Lim, Y.Y. and Chaudhi, M.M., Philos. Mag. A 79, 2979 (1999).CrossRefGoogle Scholar
7.Ma, Q. and Clarke, D.R., J. Mater. Res. 10, 853 (1995).CrossRefGoogle Scholar
8.Huang, Y., Xue, Z., Gao, H., Nix, W.D., Xia, Z.C., J Mater. Res. 15, 1786 (2000).CrossRefGoogle Scholar
9.Tymiak, N.I., Kramer, D.E., Bahr, D.F., Wyrobek, T.J., and Gerberich, W.W., Acta Mater. 49, 1024 (2001).CrossRefGoogle Scholar
10.Poole, W.J., Ashby, M.F., and Fleck, N.A., Scripta Mater. 34, 559 (1996).CrossRefGoogle Scholar
11.Bull, S.J., Page, T.F., and Yoffe, E.H., Philos. Mag. Lett. 59, 281 (1989).CrossRefGoogle Scholar
12.Li, H. and Bradt, R.C., J. Mater. Sci. 28, 917 (1993).CrossRefGoogle Scholar
13.Li, H., Han, Y.H., and Bradt, R.C., J. Mater. Sci. 29, 5641 (1994).CrossRefGoogle Scholar
14.Lee, C.S., Han, G.W., Smallman, R.E., Feng, D., and Lai, J.K.L., Acta Mater. 47, 1823 (1999).CrossRefGoogle Scholar
15.Page, T.F., Riester, L., and Hainsworth, S.V., in Fundamentals of Nanoindentation and Nanotribology, edited by Moody, N.R., Gerberich, W.W., Burnham, N., and Baker, S.P. Warrendale, Pa, (Mater. Res. Soc. Symp. Proc. Warrendale, PA, 522, 1998), 113.Google Scholar
16.Prikhodko, S.V., Carens, J.C., Isaak, D.G., and Ardell, A.J., Metal. Mater. Trans. A 30, 2403 (1999).CrossRefGoogle Scholar
17.Zhang, Y.G., Han, Y.F., Chen, G.L., Guo, Z.T., Wan, X.J., and Feng, D., Structural Intermetallics, 17, 1 (In Chinese) (2001).Google Scholar
18.Rao, P.V.M., Murthy, K.S., Suryanarayana, S.V., and Naidu, S.V.N., J. Mater. Res. 8, 741 (1993).CrossRefGoogle Scholar
19.Brusso, J.A. and Mikkola, D.E., J. Mater. Res. 9, 1742 (1994).CrossRefGoogle Scholar
20.Ashby, M.F., Philos. Mag. 21, 399 (1970).CrossRefGoogle Scholar
21.Umakoshi, Y., Pope, D.P., and Vitek, V., Acta Mater. 32, 449 (1984).CrossRefGoogle Scholar
22.Heredia, F.E. and Pope, D.P., Acta Mater. 39, 2017 (1991).CrossRefGoogle Scholar
23.Heredia, F.E. and Pope, D.P., Acta Mater. 39, 2027 (1991).CrossRefGoogle Scholar
24.Norwak, R. and Sakai, M., Acta Metall. Mater. 42, 2879 (1994).CrossRefGoogle Scholar