Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Yamaguchi, Akihiro
Murakami, Hideyuki
Kuroda, Seiji
and
Imai, Hachiro
2007.
Effect of Hf Addition on Oxidation Properties of Pt-Ir Modified Aluminide Coating.
MATERIALS TRANSACTIONS,
Vol. 48,
Issue. 9,
p.
2422.
Young, John
2008.
High Temperature Oxidation and Corrosion of Metals.
Vol. 1,
Issue. ,
p.
361.
Garimella, N.
Ode, M.
Ikeda, M.
Murakami, H.
and
Sohn, Y.H.
2008.
Effects of Ir or Ta Alloying Addition on Interdiffusion of L12–Ni3Al.
Intermetallics,
Vol. 16,
Issue. 9,
p.
1095.
Garimella, N.
Ode, M.
Ikeda, M.
Murakami, H.
and
Sohn, Y. H.
2009.
Interdiffusion in L12-Ni3Al Alloyed with Re.
Journal of Phase Equilibria and Diffusion,
Vol. 30,
Issue. 3,
Yasui, Yoshito
Murakami, Hideyuki
Yoshida, Mikiyo
Sato, Akihiro
Tateno, Akira
Kuroda, Seiji
and
Imai, Hachiro
2009.
Oxidation Resistance of Electroplated Pt-Ir Alloy Coatings on Ni-Based Single Crystal Superalloys Followed by Diffusion Annealing Treatment.
Journal of the Japan Institute of Metals,
Vol. 73,
Issue. 12,
p.
913.
Yamabe-Mitarai, Yoko
Aoyagi, Takeshi
and
Abe, Taichi
2009.
An investigation of phase separation in the Ir–Pt binary system.
Journal of Alloys and Compounds,
Vol. 484,
Issue. 1-2,
p.
327.
Song, Yingxue
Murakami, Hideyuki
and
Zhou, Chungen
2011.
Cyclic-Oxidation Behavior of Multilayered Pt/Ru-Modified Aluminide Coating.
Journal of Materials Science & Technology,
Vol. 27,
Issue. 3,
p.
280.
Bao, Z.B.
Murakami, H.
and
Yamabe-Mitarai, Y.
2011.
Surface geometry of pure iridium oxidized at 1373K in air.
Applied Surface Science,
Vol. 258,
Issue. 4,
p.
1514.
Song, Y.
Zhou, C.
and
Murakami, H.
2011.
Microstructural investigation of PGM‐based alloy coatings for oxidation protection.
Materials and Corrosion,
Vol. 62,
Issue. 7,
p.
674.
Zhou, C.G.
and
Song, Y.X.
2011.
Thermal Barrier Coatings.
p.
193.
Bao, Z.B.
Murakami, H.
and
Yamabe-Mitarai, Y.
2011.
Effects of thermal exposure on Ir-based alloys with and without Pt coating.
Corrosion Science,
Vol. 53,
Issue. 4,
p.
1224.
Xiao, W. L.
Murakami, H.
Ping, D. H.
and
Yamabe-Mitarai, Y.
2013.
Microstructure and oxidation behaviors of near-α Ti-6.5Al-4Sn-4Zr-0.5Mo-based alloys with Ir addition.
Journal of Materials Science,
Vol. 48,
Issue. 9,
p.
3363.
ALLAHYARZADEH, M. H.
ALIOFKHAZRAEI, M.
and
ROUHAGHDAM, A. SABOUR
2016.
ELECTRODEPOSITION ON SUPERALLOY SUBSTRATES: A REVIEW.
Surface Review and Letters,
Vol. 23,
Issue. 03,
p.
1630001.
Young, David J.
2016.
High Temperature Oxidation and Corrosion of Metals.
p.
393.
Bespyatov, M.A.
Kuzin, T.M.
Naumov, V.N.
Vikulova, E.S.
Ilyin, I.Yu.
Morozova, N.B.
and
Gelfond, N.V.
2016.
Low-temperature heat capacity of Ir(C5H7O2)(C8H12).
The Journal of Chemical Thermodynamics,
Vol. 99,
Issue. ,
p.
70.
Tue, Dao Chi
Tsao, Te-Kang
Ishida, Akira
Murakami, Hideyuki
and
Lien, Le Thi Hong
2020.
Microstructure and Oxidation Behavior of Pt and Pt–Ir Diffusion Coatings on Ni-Based Single Crystal Superalloy.
MATERIALS TRANSACTIONS,
Vol. 61,
Issue. 8,
p.
1671.
Zhou, Yunxuan
Yu, Wei
Chong, Xiaoyu
Wei, Yan
Hu, Changyi
Zhang, Aimin
and
Feng, Jing
2020.
Rapid screening of alloy elements to improve the elastic properties of dilute Pt-based alloys: High-throughput first-principles calculations and modeling.
Journal of Applied Physics,
Vol. 128,
Issue. 23,
Aliabadi, Ali
Mehdi Hadavi, Seyed Mohammad
and
Eshraghi, Mohamad Javad
2021.
Mechanistic investigation of aluminide coating formation by low-pressure chemical vapor deposition method on NiCoCrAlY coating in presence of nickel-ceria composite layer.
Ceramics International,
Vol. 47,
Issue. 14,
p.
20051.
Qian, Ling-Yi
Wang, Jing
Guo, Yun-Shan
Liu, He
and
Bao, Ze-Bin
2021.
Influences of Iridium and Palladium on Oxidation Resistance of PtAl Coating.
Acta Metallurgica Sinica (English Letters),
Vol. 34,
Issue. 8,
p.
1120.
Zhang, C.Y.
Li, Y.Y.
Ji, H.Z.
Zhang, C.
Niu, X.Y.
Li, S.
Bao, Z.B.
Zhu, S.L.
and
Wang, F.H.
2025.
Hot corrosion and interdiffusion behavior of refurbished (Ni,Pt)Al coating on Ni-based superalloy.
Corrosion Science,
Vol. 247,
Issue. ,
p.
112773.