Hostname: page-component-68c7f8b79f-lvtpz Total loading time: 0 Render date: 2025-12-23T01:41:43.164Z Has data issue: false hasContentIssue false

Effects of boron and zirconium additions on the fluidity, microstructure and mechanical properties of IN718C superalloy

Published online by Cambridge University Press:  21 October 2016

Ziqi Jie
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
Jun Zhang*
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
Taiwen Huang*
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
Haijun Su*
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
Yanbin Zhang
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
Lin Liu
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
Hengzhi Fu
Affiliation:
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, People's Republic of China
*
a) Address all correspondence to these authors. e-mail: zhjscott@nwpu.edu.cn
c) e-mail: shjnpu@nwpu.edu.cn
Get access

Abstract

The effects of boron and zirconium contents from 0 to 0.049 wt% on the casting fluidity, as-cast microstructure and mechanical properties of IN718C superalloy are systematically investigated. The results show that as the B or Zr content increases, the fluidity firstly increases and then decreases. The optimum fluidity is obtained at the pouring temperature of 1470 °C when the content of B is 0.0059 wt% or Zr is 0.042 wt%, respectively. The addition of Zr can lead to the formation of blocky laves phase, but B has no influence on microstructure morphology. Furthermore, the addition of B or Zr can effectively improve the tensile and stress life properties as well as casting fluidity of IN718C superalloy. As compared with IN718C master alloys, the tensile strength can increase 6.2–8.6% and stress life can be improved by 1.3 times when B content is 0.0059 wt%. In addition, when the alloy contains 0.042 wt% Zr, the tensile strength can increase 5.6–7% and stress life can increase 1.076 times than that of the master alloy.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2016 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Reed, R.C.: The Superalloys: Fundamentals and Applications (Cambridge University Press, Cambridge, 2006); p. 2.Google Scholar
Donachie, M.J. and Donachie, S.J.: Superalloys: A Technical Guide (ASM International, Materials Park, 2002); p. 211.Google Scholar
Banerjee, K.: The role of magnesium in superalloys–A Review. Mater. Sci. Appl. 2, 1243 (2011).Google Scholar
Yu, Z.H., Qiang, J.F., Zhang, J., and Liu, L.: Microstructure evolution during heat treatment of superalloys loaded with different amounts of carbon. J. Mater. Res. 30, 2064 (2015).Google Scholar
Yang, J.X., Zheng, Q., Ji, M.Q., Sun, X.F., and Hu, Z.Q.: Effects of different C contents on the microstructure, tensile properties and stress-rupture properties of IN792 alloy. Mater. Sci. Eng., A 528, 1534 (2011).Google Scholar
Sun, W.R., Guo, S.R., Lee, J.H., Park, N.K., Yoo, Y.S., Choe, S.J., and Hu, Z.Q.: Effects of phosphorus on the δ-Ni3Nb phase precipitation and the stress rupture properties in alloy 718. Mater. Sci. Eng., A 247, 173 (1998).Google Scholar
Wang, C.S., Guo, Y.A., Guo, J.T., and Zhou, L.Z.: Microstructural stability and mechanical properties of a boron modified Ni–Fe based superalloy for steam boiler applications. Mater. Sci. Eng., A 639, 380 (2015).Google Scholar
Yan, B.C., Zhang, J., and Lou, L.H.: Effect of boron additions on the microstructure and transverse properties of a directionally solidified superalloy. Mater. Sci. Eng., A 474, 39 (2008).Google Scholar
Xiao, L., Chen, D.L., and Chaturvedi, M.C.: Effect of boron on fatigue crack growth behavior in superalloy IN 718 at RT and 650 C. Mater. Sci. Eng., A 428, 1 (2006).Google Scholar
Zhou, P.J., Yu, J.J., Sun, X.F., Guan, H.R., and Hu, Z.Q.: The role of boron on a conventional nickel-based superalloy. Mater. Sci. Eng., A 491, 159 (2008).Google Scholar
Miao, Z.J., Shan, A.D., Lu, J., and Song, H.W.: Microstructure and solidification behaviour characterisation of phosphorus and boron doped IN718 superalloy. Mater. Sci. Technol. 28, 334 (2012).Google Scholar
Tsai, Y.L., Wang, S.F., Bor, H.Y., and Hu, Y.F.: Effects of Zr addition on the microstructure and mechanical behavior of a fine-grained nickel-based superalloy at elevated temperatures. Mater. Sci. Eng., A 607, 294 (2014).Google Scholar
Mostafaei, M. and Abbasi, S.M.: Influence of Zr content on the incipient melting behavior and stress-rupture life of CM247 LC nickel base superalloy. J. Alloys Compd. 648, 1031 (2015).Google Scholar
Huang, H.E. and Koo, C.H.: Effect of zirconium on microstructure and mechanical properties of cast fine-grain CM 247 LC superalloy. Mater. Trans. 45, 554 (2004).Google Scholar
Floreen, S. and Davidson, J.M.: The effects of B and Zr on the creep and fatigue crack growth behavior of a Ni-base superalloy. Metall. Trans. A 14, 895 (1983).Google Scholar
Zhang, J. and Singer, R.F.: Effect of Zr and B on castability of Ni-based superalloy IN792. Metall. Mater. Trans. A 35, 1337 (2004).Google Scholar
Campbell, J.: Castings (Butterworth-Heinemann, Oxford, 2003); p. 2.Google Scholar
Turen, Y.: Effect of Sn addition on microstructure, mechanical and casting properties of AZ91 alloy. Mater. Des. 49, 1009 (2013).Google Scholar
Sin, S.L. and Dube, D.: Influence of process parameters on fluidity of investment-cast AZ91D magnesium alloy. Mater. Sci. Eng., A 386, 34 (2004).Google Scholar
Ping, D.H., Gu, Y.F., Cui, C.Y., and Harada, H.: Grain boundary segregation in a Ni–Fe-based (Alloy 718) superalloy. Mater. Sci. Eng., A 456, 99 (2007).Google Scholar
Dong, J.X., Zhang, M.C., Xie, X.S., and Thompson, R.G.: Interfacial segregation and cosegregation behaviour in a nickel-base alloy 718. Mater. Sci. Eng., A 328, 8 (2002).Google Scholar
Xiao, L., Chen, D.L., and Chaturvedi, M.C.: Effect of boron and carbon on the fracture toughness of IN 718 superalloy at room temperature and 650° C. J. Mater. Eng. Perform. 14, 528 (2005).Google Scholar
Garosshen, T.J., Tillman, T.D., and Mccarthy, G.P.: Effects of B, C, and Zr on the structure and properties of a P/M nickel base superalloy. Metall. Trans. A 18, 69 (1987).Google Scholar
Alam, T., Felfer, P.J., Chaturvedi, M., Stephenson, L.T., Kilburn, M.R., and Cairney, J.M.: Segregation of B, P, and C in the Ni-based superalloy, inconel 718. Metall. Mater. Trans. A 43, 2183 (2012).Google Scholar
Nakagawa, Y., Ohta, T., Kaneno, Y., Inoue, H., and Takasugi, T.: Defect structures and room-temperature mechanical properties of C15 laves phases in Zr–Nb–Cr and Zr–Hf–Cr alloy systems. Metall. Mater. Trans. A 35, 3469 (2004).Google Scholar
Li, Y.M., Liu, H.J., Liu, J., Wang, Z.P., and Hao, Y.: Effect of Zr addition on precipitates in K4169 superalloy. China Foundry 9, 6 (2012).Google Scholar
Tytko, D., Choi, P.P., Klower, J., Kostka, A., Inden, G., and Raabe, D.: Microstructural evolution of a Ni-based superalloy (617B) at 700 C studied by electron microscopy and atom probe tomography. Acta Mater. 60, 1731 (2012).Google Scholar
Thuvander, M. and Stiller, K.: Microstructure of a boron containing high purity nickel-based alloy 690. Mater. Sci. Eng., A 281, 96 (2000).Google Scholar
Richards, N.L. and Chaturvedi, M.C.: Effect of minor elements on weldability of nickel base superalloys. Int. Mater. Rev. 45, 109 (2000).Google Scholar
Bae, J.S., Lee, J.H., Kim, S.S., and Jo, C.Y.: Formation of MC-γ/γ′ eutectic fibers and their effect on stress rupture behavior in D/S Mar-M247LC superalloy. Scripta Mater. 45, 503 (2001).Google Scholar
Chen, J., Lee, J.H., Jo, C.Y., Choe, S.J., and Lee, Y.T.: MC carbide formation in directionally solidified MAR-M247 LC superalloy. Mater. Sci. Eng., A 247, 113 (1998).Google Scholar
Yang, J.X., Zheng, Q., Sun, X.F., Guan, H.G., and Hu, Z.Q.: Relative stability of carbides and their effects on the properties of K465 superalloy. Mater. Sci. Eng., A 429, 341 (2006).Google Scholar