Surface Structural Characterization and Mechanical Testing by Nanoindentation Measurements of Hybrid Polymer/clay Nanostructured Multilayer Films

Published online by Cambridge University Press:  31 January 2011

Xiaowu Fan
Affiliation:
Alabama Tri-campus Materials Science Program and Department of Chemistry, University of Alabama at Birmingham, Birmingham, Alabama 35294–1240
Mi-Kyoung Park
Affiliation:
Department of Chemistry, University of Alabama at Birmingham, Birmingham, Alabama 35294–1240
Chuanjun Xia
Affiliation:
Department of Chemistry, University of Alabama at Birmingham, Birmingham, Alabama 35294–1240
Rigoberto Advincula*
Affiliation:
Alabama Tri-campus Materials Science Program and Department of Chemistry, University of Alabama at Birmingham, Birmingham, Alabama 35294–1240
*
a)Address all correspondence to this author.
Get access

Abstract

Nanostructured montmorillonite/poly(diallyldimethylammonium chloride) multilayer thin films were fabricated up to 100 layers thick by stepwise alternating polyelectrolyte and clay deposition from solution. The structure and morphology of the films were characterized by x-ray diffraction, ellipsometry, atomic force microscopy, and quartz crystal microbalance ex situ and in situ measurements. The mechanical properties were tested by nanoindentation. The hardness of the multilayer thin film was 0.46 GPa. The thin film's modulus was correlated to its ordering and anisotropic structure. Both hardness and modulus of this composite film were higher than those of several other types of polymer thin films.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

Fendler, J.H., Chem. Mater. 8, 1616 (1996).Google Scholar
Decher, G., Science 277, 1232 (1997).CrossRefGoogle Scholar
He, J-A., Samuelson, L., Li, L., Kumar, J., and Tripathy, S.K., Langmuir 14, 1674 (1998).Google Scholar
Giannelis, E.P., Krishnamoorti, R., and Manias, E., Adv. Polym. Sci. 138, 107 (1999).Google Scholar
Kleinfeld, E.R. and Ferguson, G.S., Science 265, 370 (1994).Google Scholar
Kotov, N.A., Haraszti, T., Turi, L., Zavala, G., Geer, R.E., Dekany, I., and Fendler, J.H., J. Am. Chem. Soc. 119, 6821 (1997).Google Scholar
Kleinfeld, E.R. and Ferguson, G.S., Chem. Mater. 8, 1575 (1996).Google Scholar
Duffel, B. Van, Schoonheydt, R.A., Grim, C.P.M., and DeSchryver, F.C., Langmuir 15, 7520 (1999).Google Scholar
Kotov, N.A., Magonov, S., and Tropsha, E., Chem. Mater. 10, 886 (1998).CrossRefGoogle Scholar
Kim, D.W., Blumstein, A., Kuma, J., and Tripathy, K.S., Chem. Mater. Commun. 13, 565 (2001).Google Scholar
Kleinfeld, E.R. and Ferguson, G.S., Chem. Mater. 7, 2327 (1995).CrossRefGoogle Scholar
Tillman, N., Ulman, A., and Penner, L.T., Langmuir 5, 101 (1989).Google Scholar
Sauerbrey, G.Z., Physik. 155, 206 (1959).Google Scholar
Lvov, Y., Ariga, K., Ichinose, I., and Kunitake, T., Langmuir 12, 3038 (1996).Google Scholar
Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, 1564 (1992).Google Scholar
Li, J., Thostenson, E.T., Chou, T.W., and Riester, L.J., Eng. Mater. Technol. 120, 154 (1998).CrossRefGoogle Scholar
Mann, A.B. and Pethica, J.B., Langmuir 12, 4583 (1996).Google Scholar
Poilane, C., Delobelle, P., Lexcellent, C., Hayashi, S., and Tobushi, H., Thin Sold Film 379, 156 (2000).Google Scholar
Karapanagotis, I., Gerberich, W.W., and Evans, D.F., Langmuir 17, 2375 (2001).CrossRefGoogle Scholar
Wang, J., Shi, F.G., Nieh, T.G., Zhao, B., Brongo, M.R., Qu, S., and Rosenmayer, T., Scripta Mater. 42, 687 (2000).CrossRefGoogle Scholar
Gracias, D. and Somorjai, G., Macromolecules 31, 1269 (1998).Google Scholar
Domke, J. and Radmacher, M., Langmuir 14, 3320 (1998).Google Scholar
Du, B., Tsui, O.K., Zhang, Q., and He, T., Langmuir 17, 3286 (2001).CrossRefGoogle Scholar