Hostname: page-component-68c7f8b79f-lqrcg Total loading time: 0 Render date: 2025-12-19T08:34:28.893Z Has data issue: false hasContentIssue false

On anomalous depth-dependency of the hardness of NiTi shape memory alloys in spherical nanoindentation

Published online by Cambridge University Press:  09 July 2013

Wenyi Yan*
Affiliation:
Department of Mechanical & Aerospace Engineering, Monash University, Clayton, Victoria 3800, Australia
Abbas Amini
Affiliation:
Institute for Frontier Materials, Deakin University, Waurn Ponds, Victoria 3217, Australia
Qingping Sun
Affiliation:
Department of Mechanical Engineering, The Hong Kong University of Science and Technology, Kowloon, Hong Kong, China
*
a)Address all correspondence to this author. e-mail: wenyi.yan@monash.edu
Get access

Abstract

An experimental study on the indentation hardness of NiTi shape memory alloys (SMAs) by using a spherical indenter tip and a finite element investigation to understand the experimental results are presented in this paper. It is shown that the spherical indentation hardness of NiTi SMAs increases with the indentation depth. The finding is contrary to the recent study on the hardness of NiTi SMAs using a sharp Berkovich indenter tip, where the interfacial energy plays a dominant role at small indentation depths. Our numerical investigation indicates that the influence of the interfacial energy is not significant on the spherical indentation hardness of SMAs. Furthermore, the depth dependency of SMA hardness under a spherical indenter is explained by the elastic spherical contact theory incorporating the deformation effect of phase transformation of SMAs. Hertz theory for purely elastic contact shows that the spherical hardness increases with the square root of the indentation depth. The phase transformation beneath the spherical tip weakens the depth effect of a purely elastic spherical hardness. This study enriches our knowledge on the basic concept of hardness for SMAs under spherical indentation at micro- and nanoscales.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2013 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Archard, J.F.: Contact and rubbing of flat surfaces. J. Appl. Phys. 24, 981 (1953).CrossRefGoogle Scholar
Tabor, D.: The Hardness of Metals, 1st ed. (Oxford Press, London, England, 1951), p. 85.Google Scholar
Cheng, Y.T. and Cheng, C.M.: What is indentation hardness? Surf. Coat. Technol. 133134, 417 (2000).CrossRefGoogle Scholar
Cheng, Y.T. and Cheng, C.M.: Scaling, dimensional analysis, and indentation measurements. Mater. Sci. Eng., R. 44, 91 (2004).CrossRefGoogle Scholar
Ma, Q. and Clarke, D.R.: Size dependent hardness of silver single crystals. J. Mater. Res. 10, 853 (1995).CrossRefGoogle Scholar
McElhaney, K.W., Vlassk, J.J., and Nix, W.D.: Determination of indenter tip geometry and indentation contact area for depth sensing indentation experiments. J. Mater. Res. 13, 1300 (1998).CrossRefGoogle Scholar
Nix, W.D. and Gao, H.: Indentation size effects in crystalline materials: A law of strain gradient plasticity. J. Mech. Phys. Solids 46, 411 (1998).CrossRefGoogle Scholar
Huang, Y., Zhang, F., Hwang, K.C., Nix, W.D., Pharr, G.M., and Feng, G.: A model of size effects in nano-indentation. J. Mech. Phys. Solids 54, 1668 (2006).CrossRefGoogle Scholar
Swadener, J.G., George, E.P., and Pharr, G.M.: The correlation of the indentation size effect measured with indenters of various shapes. J. Mech. Phys. Solids 50, 681 (2002).CrossRefGoogle Scholar
Shaw, G.A., Trethewey, J.S., Johnson, A.D., Drugan, W.J., and Crone, W.C.: Thermomechanical high-density data storage in a metallic material via the shape-memory effect. Adv. Mater. 17, 1123 (2005).CrossRefGoogle Scholar
Satoh, G., Birnbaum, A., and Yao, Y.L.: Annealing effect on the shape memory properties of amorphous NiTi thin films. J. Manuf. Sci. Eng. 132, 051004 (2010).CrossRefGoogle Scholar
Li, Y-H., Rao, G-B., Rong, L-J., and Li, Y-Y.: The influence of porosity on corrosion characteristics of porous NiTi alloy in simulated body fluid. Mater. Lett. 57, 448 (2002).CrossRefGoogle Scholar
Shaw, G.A., Stone, D.S., Johnson, A.D., Ellis, A.B., and Crone, W.C.: Shape memory effect in nanoindentation of nickel–titanium thin films. Appl. Phys. Lett. 83, 257 (2003).CrossRefGoogle Scholar
Ni, W., Cheng, Y.T., and Grummon, D.S.: Microscopic shape memory and superelastic effects under complex loading conditions. Surf. Coat. Technol. 177178, 512 (2004).CrossRefGoogle Scholar
Ma, X-G. and Komvopoulos, K.: Pseudoelasticity of shape-memory titanium–nickel films subjected to dynamic nanoindentation. Appl. Phys. Lett. 84, 4274 (2004).CrossRefGoogle Scholar
Huang, W.M., Su, J.F., Hong, M.H., and Yang, B.: Pile-up and sink-in in micro-indentation of a NiTi shape-memory alloy. Scr. Mater. 53, 1055 (2005).CrossRefGoogle Scholar
Amini, A., Yan, W., and Sun, Q.: Depth dependency of indentation hardness during solid-state phase transition of shape memory alloys. Appl. Phys. Lett. 99, 021901 (2011).CrossRefGoogle Scholar
Amini, A., He, Y., and Sun, Q.: Loading rate dependency of maximum nanoindentation depth in nano-grained NiTi shape memory alloy. Mater. Lett. 65, 464 (2011).CrossRefGoogle Scholar
Oliver, W.C. and Pharr, G.M.: An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7, 1564 (1992).CrossRefGoogle Scholar
Yan, W., Sun, Q., and Liu, H-Y.: Effect of transformation volume strain on the spherical indentation of shape memory alloys. Int. J. Mod. Phys. B 22, 5957 (2008).CrossRefGoogle Scholar
Kang, G. and Yan, W.: Effects of phase transition on the hardness of shape memory alloys. Appl. Phys. Lett. 94, 261906 (2009).CrossRefGoogle Scholar
Kang, G. and Yan, W.: Scaling relationships in sharp conical indentation of shape memory alloys. Philos. Mag. 90, 599 (2010).CrossRefGoogle Scholar
Yan, W., Sun, Q., and Liu, H.-Y.: Spherical indentation hardness of shape memory alloys. Mater. Sci. Eng., A 425, 278 (2006).CrossRefGoogle Scholar
Johnson, K.L.: Contact Mechanics (Cambridge University Press, Cambridge, England, 1985), p. 100.CrossRefGoogle Scholar
Qian, L., Xiao, X., Sun, Q., and Yu, T.: Anomalous relationship between hardness and wear properties of a superelastic nickel-titanium alloy. Appl. Phys. Lett. 84, 1076 (2004).CrossRefGoogle Scholar