Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Shibata, Akinobu
Nagoshi, Takashi
Sone, Masato
Morito, Shigekazu
and
Higo, Yakichi
2010.
Evaluation of the block boundary and sub-block boundary strengths of ferrous lath martensite using a micro-bending test.
Materials Science and Engineering: A,
Vol. 527,
Issue. 29-30,
p.
7538.
Voyiadjis, G Z
and
Faghihi, D
2010.
Variable (intrinsic) material length scale for face-centred cubic metals using nano-indentation.
Proceedings of the Institution of Mechanical Engineers, Part N: Journal of Nanoengineering and Nanosystems,
Vol. 224,
Issue. 3,
p.
123.
QiJia Chen
Pagba, Ariel
Reynoso, Dexter
Thomas, Sven
and
Toc, Howell John
2010.
Cu wire and beyond - Ag wire an alternative to Cu?.
p.
591.
Ramos, K.J.
Bahr, D.F.
and
Hooks, D.E.
2011.
Defect and surface asperity dependent yield during contact loading of an organic molecular single crystal.
Philosophical Magazine,
Vol. 91,
Issue. 7-9,
p.
1276.
Sekido, Kaoru
Ohmura, Takahito
Hara, Toru
and
Tsuzaki, Kaneaki
2012.
Effect of Dislocation Density on the Initiation of Plastic Deformation on Fe–C Steels.
MATERIALS TRANSACTIONS,
Vol. 53,
Issue. 5,
p.
907.
Faghihi, Danial
and
Voyiadjis, George Z.
2012.
Determination of nanoindentation size effects and variable material intrinsic length scale for body-centered cubic metals.
Mechanics of Materials,
Vol. 44,
Issue. ,
p.
189.
Armstrong, R. W.
and
Elban, W. L.
2012.
Hardness properties across multiscales of applied loads and material structures.
Materials Science and Technology,
Vol. 28,
Issue. 9-10,
p.
1060.
Pathak, Siddhartha
Michler, Johann
Wasmer, Kilian
and
Kalidindi, Surya R.
2012.
Studying grain boundary regions in polycrystalline materials using spherical nano-indentation and orientation imaging microscopy.
Journal of Materials Science,
Vol. 47,
Issue. 2,
p.
815.
Benjamin Britton, T.
and
Wilkinson, Angus J.
2012.
Stress fields and geometrically necessary dislocation density distributions near the head of a blocked slip band.
Acta Materialia,
Vol. 60,
Issue. 16,
p.
5773.
Ohmura, T.
Zhang, L.
Sekido, K.
and
Tsuzaki, K.
2012.
Effects of lattice defects on indentation-induced plasticity initiation behavior in metals.
Journal of Materials Research,
Vol. 27,
Issue. 13,
p.
1742.
Stewart, J. L.
Williams, J. J.
and
Chawla, N.
2012.
Influence of Thermal Aging on the Microstructure and Mechanical Behavior of Dual-Phase, Precipitation-Hardened, Powder Metallurgy Stainless Steels.
Metallurgical and Materials Transactions A,
Vol. 43,
Issue. 1,
p.
124.
Stegall, David E.
Mamun, Md. Abdullah
Crawford, Bryan
and
Elmustafa, Abdelmageed
2012.
Indentation size effect in FCC metals: An examination of experimental techniques and the bilinear behavior.
Journal of Materials Research,
Vol. 27,
Issue. 12,
p.
1543.
Jiang, J.
Britton, T.B.
and
Wilkinson, A.J.
2013.
Measurement of geometrically necessary dislocation density with high resolution electron backscatter diffraction: Effects of detector binning and step size.
Ultramicroscopy,
Vol. 125,
Issue. ,
p.
1.
OHMURA, Takahito
2013.
Prospects of Nanoindentation and Related Techniques.
Journal of the Japan Society for Precision Engineering,
Vol. 79,
Issue. 12,
p.
1181.
ARMSTRONG, R. W.
ELBAN, W. L.
and
WALLEY, S. M.
2013.
ELASTIC, PLASTIC, CRACKING ASPECTS OF THE HARDNESS OF MATERIALS.
International Journal of Modern Physics B,
Vol. 27,
Issue. 08,
p.
1330004.
OHMURA, Takahito
2013.
Evaluation of Mechanical Properties by Nano-scale Characterization.
Journal of the Japan Society for Technology of Plasticity,
Vol. 54,
Issue. 633,
p.
886.
Voyiadjis, George Z.
and
Faghihi, Danial
2013.
Gradient plasticity for thermo-mechanical processes in metals with length and time scales.
Philosophical Magazine,
Vol. 93,
Issue. 9,
p.
1013.
Shibata, Akinobu
Nagoshi, Takashi
Sone, Masato
and
Higo, Yakichi
2013.
Micromechanical characterization of deformation behavior in ferrous lath martensite.
Journal of Alloys and Compounds,
Vol. 577,
Issue. ,
p.
S555.
Faghihi, Danial
Voyiadjis, George Z.
and
Park, Taehyo
2013.
Coupled Thermomechanical Modeling of Small Volume FCC Metals.
Journal of Engineering Materials and Technology,
Vol. 135,
Issue. 2,
Ohmura, Takahito
2013.
Analysis of local deformation behavior in metallic materials through nanoindentation technique.
Journal of Japan Institute of Light Metals,
Vol. 63,
Issue. 2,
p.
65.