Hostname: page-component-68c7f8b79f-tw422 Total loading time: 0 Render date: 2025-12-19T14:14:21.612Z Has data issue: false hasContentIssue false

Illustrative analysis of load-displacement curves in nanoindentation

Published online by Cambridge University Press:  31 January 2011

A.C. Fischer-Cripps*
Affiliation:
Industrial Physics, Commonwealth Scientific and Industrial Research Organization (CSIRO), West Lindfield, New South Wales, 2070 Australia
*
a)Address all correspondence to this author. e-mail: tony.cripps@csiro.au
Get access

Abstract

The nature of the elastic unloading after an elastic-plastic contact with a conical or Berkovich indenter is studied. Three representative specimens having different mechanical properties were tested. Finite-element results for the pressure distribution beneath the indenter during unloading suggest that the effective indenter is in fact very closely approximated by a sphere in the case of fused silica (a material with a relatively low value of E/H) and a more uniform pressure distribution in the case of silicon and sapphire (materials with higher values of E/H). The proposed reason for these observations is the extent and influence of an elastic enclave directly beneath the indenter as revealed by finite-element analysis. The results also show that the pressure distribution retains its form during the entire unloading. The work seeks to provide a physical reason for the value of the fitting exponent m as used in popular nanoindentation data analysis procedures.

Keywords

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1Oliver, W.C.Pharr, G.M.: An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7(4), 1664 1992CrossRefGoogle Scholar
2Pharr, G.M.Bolshakov, A.: Understanding nanoindentation unloading curves. J. Mater. Res. 17(10), 2660 2002Google Scholar
3Cheng, Y-T.Cheng, C-M.: Scaling, dimensional analysis, and indentation measurements. Mater. Sci. Eng., R 44, 99 2004CrossRefGoogle Scholar
4Fischer-Cripps, A.C.Nanoindentation, 2nd ed.Springer Verlag New York 2004CrossRefGoogle Scholar
5Fischer-Cripps, A.C.: The use of combined elastic modulus in depth-sensing indentation with a conical indenter. J. Mater. Res. 18(5), 1043 2003Google Scholar
6Sneddon, I.N.: Boussinesq’s problem for a rigid cone. Proc. Cambridge Philos. Soc. 44, 492 1948Google Scholar
7Gong, J., Miao, H.Peng, Z.: A new function for the description of the nanoindentation unloading data. Scripta Mater. 49(1), 93 2003CrossRefGoogle Scholar
8Fischer-Cripps, A.C.: Elastic recovery and reloading of hardness impressions with a conical indenter in Surface Engineering 2002—Synthesis, Characterization and Applications, edited by A. Kumar, W.J. Meng, Y-T. Cheng, J.S. Zabinski, G.L. Doll, and S. Veprek Mater. Res. Soc. Symp. Proc. 750, Warrendale, PA 2003 Y6.9.1Google Scholar
9Woirgard, J.Dargenton, J-C.: An alternative method for penetration depth determination in nanoindentation measurements. J. Mater. Res. 12(9), 2455 1997CrossRefGoogle Scholar
10Sneddon, I.N.: The relation between load and penetration in the axisymmetric Boussinesq problem for a punch of arbitrary profile. Int. J. Eng. Sci. 3, 47 1965Google Scholar
11Pharr, G.M., Oliver, W.C.Brotzen, F.R.: On the generality of the relationship among contact stiffness, contact area, and the elastic modulus during indentation. J. Mater. Res. 7(3), 613 1992Google Scholar
12Cheng, Y-T., Li, Z.Cheng, C-M.: Scaling relationships for indentation measurements. Philos. Mag. A 82, 1821 2002CrossRefGoogle Scholar
13Tho, K.K., Swaddiwudhipong, S., Liu, Z.S., Zeng, K.Hua, J.: Uniqueness of reverse analysis from conical indentation tests. J. Mater. Res. 19(8), 2498 2004CrossRefGoogle Scholar