Hostname: page-component-68c7f8b79f-qcl88 Total loading time: 0 Render date: 2025-12-23T08:41:21.146Z Has data issue: false hasContentIssue false

Fundamental relations used in nanoindentation: Critical examination based on experimental measurements

Published online by Cambridge University Press:  31 January 2011

M. Martin
Affiliation:
Unité de Thermique et Analyse Physique, EA 2061, Université de Reims, 21, rue Clément Ader, 51685 Reims Cedex 2, France
M. Troyon
Affiliation:
Unité de Thermique et Analyse Physique, EA 2061, Université de Reims, 21, rue Clément Ader, 51685 Reims Cedex 2, France
Get access

Abstract

The fundamental relations used in the analysis of nanoindentation load–displacement data to determine elastic modulus and hardness are based on Sneddon's solution for indentation of an elastic half-space by rigid axisymmetric indenters. It has been recently emphasized that several features that have important implications for nanoindentation measurements are generally ignored. The first one concerns the measurement of the contact depth, which is actually determined by using a constant value ε = 0.75 for the geometry of a Berkovich indenter and for any kind of material, whereas the reality is that ε is a function of the power law exponent deduced from the analysis of the unloading curve. The second feature concerns the relation between contact stiffness, elastic modulus, and contact area, in which a correction factor γ larger than unity is usually ignored leading to a systematic overestimation of the area function and thus to errors in the measured hardness and modulus. Experimental measurements on fused quartz are presented that show the variation of ε with the geometry of the tip–sample contact; that is to say with the contact depth, as well as the existence of the correction factor γ, as predicted in some recent articles. Effects of both ε and γ on harness and modulus measurements are also shown.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Pethica, J.B., Huthchings, R., and Oliver, W.C., Philos. Mag A 48, 593 (1983).Google Scholar
2.Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, 1564 (1992).CrossRefGoogle Scholar
3.Loubet, J.L., Georges, J.M., Marchesini, O., and Meille, G., J. Tribology 106, 43 (1984).Google Scholar
4.Doerner, M.F. and Nix, W.D., J. Mater. Res. 1, 601 (1986).Google Scholar
5.Sneddon, I.N., Int. J. Eng. Sci. 3, 47 (1965).Google Scholar
6.Bolshakov, A. and Pharr, G.M., J. Mater. Res. 13, 1049 (1998).Google Scholar
7.Cheng, Y-T. and Cheng, C-M., Philos. Mag. Lett. 78, 115 (1998).Google Scholar
8.Hay, J.C., Bolshakov, A., and Pharr, G.M., J. Mater. Res. 14, 2296 (1999).Google Scholar
9.Cheng, Y-T. and , C-M. Cheng, J. Appl. Phys. 84, 1284 (1998).Google Scholar
10.Dao, M., Chollacoop, N., K.J. Van Vliet, T.A. Venkatesh, and S. Suresh, Acta. Mater. 49, 3899 (2001).Google Scholar
11.Woirgard, J. and Dargenton, J.C., J. Mater. Res. 12, 2455 (1996).CrossRefGoogle Scholar
12.Cheng, Y-T. and Cheng, C-M., J. Mater. Res. 13, 1059 (1998).CrossRefGoogle Scholar