Hostname: page-component-68c7f8b79f-7wx25 Total loading time: 0 Render date: 2025-12-19T09:37:00.089Z Has data issue: false hasContentIssue false

Characteristics of metadynamic recrystallization of Nimonic 80A superalloy

Published online by Cambridge University Press:  06 February 2015

Sendong Gu
Affiliation:
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023, China
Chi Zhang
Affiliation:
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023, China
Liwen Zhang*
Affiliation:
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023, China
Wenfei Shen
Affiliation:
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023, China
*
a)Address all correspondence to this author. e-mail: commat@mail.dlut.edu.cn
Get access

Abstract

The metadynamic recrystallization (MDRX) behaviors in deformed Nimonic 80A superalloy were investigated by isothermal interrupted hot compression tests on a Gleeble-1500 thermo-mechanical simulator. Compression tests were performed using double hit schedules in the deformation temperature range of 1050–1150 °C, the interpass time range of 0.5–10 s, the strain rate range of 0.01–4 s−1, and the prestrain range of 0.30–0.50. To characterize the MDRX behaviors of the alloy, the effects of deformation temperature, strain rate, and prestrain on the metadynamic softening and recrystallized grain size were analyzed. The results reveal that the effects of deformation temperature and strain rate on the metadynamic softening fraction and recrystallized grain size are significant. However, the effects of prestrain on the metadynamic softening fraction and recrystallized grain size are not very marked and can be neglected. Then, by regression analysis of the experimental data, the MDRX kinetic model and recrystallized grain size model were proposed. The predicted results show good agreement with the experimental ones, which indicates that the proposed models can give an accurate prediction of the softening behaviors and microstructural evolution for Nimonic 80A.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2015 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Xu, Y.L., Yang, C.X., Ran, Q.X., Hu, P.F., Xiao, X.S., Cao, X.L., and Jia, G.Q.: Microstructure evolution and stress-rupture properties of Nimonic 80A after various heat treatments. Mater. Des. 47, 218226 (2013).Google Scholar
Xu, Y.L., Jin, Q.M., Xiao, X.S., Cao, X.L., Jia, G.Q., Zhu, Y.M., and Yin, H.J.: Strengthening mechanisms of carbon in modified nickel-based superalloy Nimonic 80A. Mater. Sci. Eng., A 528(13–14), 46004607 (2011).CrossRefGoogle Scholar
Jeong, H.S., Cho, J.R., and Park, H.C.: Microstructure prediction of Nimonic 80A for large exhaust valve during hot closed die forging. J. Mater. Process. Technol. 162163, 504511 (2005).Google Scholar
Wilthan, B., Preis, K., Tanzer, R., Schützenhöfer, W., and Pottlacher, G.: Thermophysical properties of the Ni-based alloy Nimonic 80A up to 2400 K, II. J. Alloys Compd. 452(1), 102104 (2008).CrossRefGoogle Scholar
Wilthan, B., Tanzer, R., Schützenhöfer, W., and Pottlacher, G.: Thermophysical properties of the Ni-based alloy Nimonic 80A up to 2400K, III. Thermochim. Acta 465(1–2), 8387 (2007).Google Scholar
Bombac, D., Brojan, M., Tercelj, M., and Turk, R.: Response to hot deformation conditions and microstructure development of Nimonic 80A superalloy. Mater. Manuf. Processes 24(6), 644648 (2009).Google Scholar
Tian, B.H., Lind, C., Schafler, E., and Paris, O.: Evolution of microstructures during dynamic recrystallization and dynamic recovery in hot deformed Nimonic 80a. Mater. Sci. Eng., A 367(1–2), 198204 (2004).Google Scholar
Kazeminezhad, M.: On the modeling of the static recrystallization considering the initial grain size effects. Mater. Sci. Eng., A 486(1–2), 202207 (2008).Google Scholar
Rao, K.P., Prasad, Y.K.D.V., and Hawbolt, E.B.: Study of fractional softening in multi-stage hot deformation. J. Mater. Process. Technol. 77(1), 166174 (1998).CrossRefGoogle Scholar
Chen, F. and Cui, Z.S.: Mesoscale simulation of microstructure evolution during multi-stage hot forging processes. Modell. Simul. Mater. Sci. Eng. 20(4), 045008(pp. 16) (2012).Google Scholar
Serajzadeh, S.: A study on kinetics of static and metadynamic recrystallization during hot rolling. Mater. Sci. Eng., A 448(1–2), 146153 (2007).Google Scholar
Gu, S.D., Zhang, L.W., Yue, C.X., Ruan, J.H., Zhang, J.L., and Gao, H.J.: Multi-field coupled numerical simulation of microstructure evolution during the hot rolling process of GCr15 steel rod. Comput. Mater. Sci. 50(7), 19511957 (2011).Google Scholar
Solhjoo, S. and Ebrahimi, R.: Prediction of no-recrystallization temperature by simulation of multi-pass flow stress curves from single-pass curves. J. Mater. Sci. 45(21), 59605966 (2010).Google Scholar
Roucoules, C., Yue, S., and Jonas, J.J.: Effect of alloying elements on metadynamic recrystallization in HSLA steels. Metall. Mater. Trans. A 26(1), 181190 (1995).Google Scholar
Cho, S.H. and Yoo, Y.C.: Determination of the metadynamic recrystallization parameter for AISI 304 stainless steel. J. Mater. Sci. Lett. 18(12), 987989 (1999).Google Scholar
Hodgson, P.D.: Microstructure modelling for property prediction and control. J. Mater. Process. Technol. 60(1), 2733 (1996).Google Scholar
Djaic, R.A.P. and Jonas, J.J.: Recrystallization of high carbon steel between intervals of high temperature deformation. Met. Trans. 4(2), 621624 (1973).CrossRefGoogle Scholar
Jung, K.H., Lee, H.W., and Im, Y.T.: Numerical prediction of austenite grain size in a bar rolling process using an evolution model based on a hot compression test. Mater. Sci. Eng., A 519(1–2), 94104 (2009).Google Scholar
Elwazri, A.M., Wanjara, P., and Yue, S.: Dynamic recrystallization of austenite in microalloyed high carbon steels. Mater. Sci. Eng., A 339, 209215 (2003).Google Scholar
Ma, B., Peng, Y., Liu, Y.F., and Jia, B.: Modeling of metadynamic recrystallization kinetics after hot deformation of low-alloy steel Q345B. J. Cent. South Univ. Technol. 17, 911917 (2010).Google Scholar
Lin, Y.C., Chen, M.S., and Zhong, J.: Study of metadynamic recrystallization behaviors in a low alloy steel. J. Mater. Process. Technol. 209(5), 24772482 (2009).Google Scholar
Lin, Y.C. and Chen, M.S.: Study of microstructural evolution during metadynamic recrystallization in a low-alloy steel. Mater. Sci. Eng., A 501(1–2), 229234 (2009).Google Scholar
Lin, Y.C., Li, L.T., and Xia, Y.C.: A new method to predict the metadynamic recrystallization behavior in 2124 aluminum alloy. Comput. Mater. Sci. 50(7), 20382043 (2011).Google Scholar
Liu, J., Liu, Y.G., Lin, H., and Li, M.Q.: The metadynamic recrystallization in the two-stage isothermal compression of 300M steel. Mater. Sci. Eng., A 565, 126131 (2013).CrossRefGoogle Scholar
Cheng, L., Chang, H., Tang, B., Kou, H.C., and Li, J.S.: Characteristics of metadynamic recrystallization of a high Nb containing TiAl alloy. Mater. Lett. 92, 430432 (2013).CrossRefGoogle Scholar
Yue, C.X., Zhang, L.W., Liao, S.L., and Gao, H.J.: Mathematical models for predicting the austenite grain size in hot working of GCr15 steel. Comput. Mater. Sci. 45(2), 462466 (2009).CrossRefGoogle Scholar
Yanagida, A. and Yanagimoto, J.: Formularization of softening fractions and related kinetics for static recrystallization using inverse analysis of double compression test. Mater. Sci. Eng., A 487(1–2), 510517 (2008).Google Scholar
Dehghan-Manshadi, A., Barnett, M.R., and Hodgson, P.D.: Hot deformation and recrystallization of austenitic stainless steel: Part II. Post-deformation recrystallization. Metall. Mater. Trans. A 39(6), 13711381 (2008).CrossRefGoogle Scholar
Choi, S. and Lee, Y.: A new approach to predicting partial recrystallization in the multi-pass hot rolling process. Met. Mater. Int. 8(1), 1523 (2002).Google Scholar
Chen, F., Cui, Z.S., Sui, D.S., and Fu, B.: Recrystallization of 30Cr2Ni4MoV ultra-super-critical rotor steel during hot deformation. Part III: Metadynamic recrystallization. Mater. Sci. Eng., A 540, 4654 (2012).Google Scholar