Analysis of thin films exhibiting large plastic deformation during nanoindentation: A modified Winkler approach

Published online by Cambridge University Press:  23 June 2015

Benjamin Boesl*
Affiliation:
Nanomechanics and Nanotribology Lab, Department of Mechanical and Materials Engineering, Florida International University, Miami, Florida 33174, USA
Gerald R. Bourne
Affiliation:
George S. Ansell Department of Metallurgical and Materials Engineering, Colorado School of Mines, Golden, Colorado 80401, USA
*
a)Address all correspondence to this author. e-mail: bboesl@fiu.edu
Get access

Abstract

A novel method for the analysis of the mechanical properties of thin films is presented and uses a modified Winkler (bed of springs) approach to estimate indentation hardness and reduced modulus using nanoindentation data. This method is especially useful in situations where significant plastic deformation occurs in the thin film resulting in pileup of material and a divergence from accepted tip area calculations. The model has been adapted into a MATLAB® script and its derivation is presented. A proof of concept study was completed using Au thin films over a range of thickness and deposition methods. Results are compared with traditional nanoindentation analysis methods and validated against the Hall–Petch relationship. It can be seen that this modified Winkler approach accurately predicts material pile-up as well as contact area for films up to 500 nm in thickness.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2015 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Jung, Y., Lawn, B., Martyniuk, M., Huang, H., and Hu, X.: Evaluation of elastic modulus and hardness of thin films by nanoindentation. J. Mater. Res. 19(10), 30763080 (2004).CrossRefGoogle Scholar
Beegan, D., Chowdhury, S., and Laugier, M.: The nanoindentation behaviour of hard and soft films on silicon substrates. Thin Solid Films 466(1–2), 167174 (2004).CrossRefGoogle Scholar
Oliver, W.C. and Pharr, G.M.: An improved technique for determining hardness and elastic-modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7(6), 15641583 (1992).CrossRefGoogle Scholar
Saha, R. and Nix, W.D.: Soft films on hard substrates – Nanoindentation of tungsten films on sapphire substrates. Mater. Sci. Eng., A 319321, 898901 (2001).CrossRefGoogle Scholar
Bolshakov, A. and Pharr, G.M.: Influence of pileup on the measurement of mechanical properties by load and depth sensing indentation techniques. J. Mater. Res. 13(4), 10491058 (1997).CrossRefGoogle Scholar
Fischer-Cripps, A.: Critical review of analysis and interpretation of nanoindentation test data. Surf. Coat. Technol. 200(14–15), 41534165 (2005).CrossRefGoogle Scholar
Põdra, P. and Andersson, S.: Wear simulation with the Winkler surface model. Wear 207(1–2), 7985 (1997).CrossRefGoogle Scholar
Jang, D.S. and Kim, D.E.: Tribological behavior of ultra-thin soft metallic deposits on hard substrates. Wear 196(1–2), 171193 (1996).CrossRefGoogle Scholar
Bourne, G.: A Methodology for Tribological Examination of Thin Films in the Nanodisplacement Regime. (ProQuest Dissertations and Theses, Florida, 2006).Google Scholar
Brandes, E.A. and Brook, G.B. eds.: Smithell's Metals Reference Book, 7th ed. (Butterworth-Heinemann, Oxford, 1998).Google Scholar
Jakes, J.E., Frihart, C.R., Beecher, J.F., Moon, R.J., and Stone, D.S.: Experimental method to account for structural compliance in nanoindentation measurements. J. Mater. Res. 23(4), 11131127 (2008).CrossRefGoogle Scholar
Stone, D.S., Yoder, K.B., and Sproul, W.D.: Hardness and elastic modulus of tin based on continuous indentation technique and new correlation. J. Vac. Sci. Tech. A 9(4), 25432547 (1991).CrossRefGoogle Scholar
Spalvins, T. and Buzek, B.: Frictional and morphological characteristics of ion-plated soft metallic films. Thin Solid Films 84(3), 267272 (1981).CrossRefGoogle Scholar
Nye, J.F.: Physical Properties of Crystals (Claredon Press, Oxford, 1998).Google Scholar
Hebbache, M.: Nanoindentation: Depth dependence of silicon hardness studied within contact theory. Phys. Rev. B 68(12), 125310 (2003).CrossRefGoogle Scholar
Kelly, A.: Strong Solids (Oxford University Press, Oxford, 1966).Google Scholar
Dieter, G.E.: Mechanical Metallurgy (McGraw-Hill, New York, 1986).Google Scholar
Conrad, H. and Jung, K.: Effect of grain size from mm to nm on the flow stress and plastic deformation kinetics of Au at low homologous temperatures. Mater. Sci. Eng., A 406(1–2), 78 (2005).CrossRefGoogle Scholar