Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Lim, Yong Yee
and
Chaudhri, M. Munawar
1999.
The effect of the indenter load on the nanohardness of ductile metals: An experimental study on polycrystalline work-hardened and annealed oxygen-free copper.
Philosophical Magazine A,
Vol. 79,
Issue. 12,
p.
2979.
Malzbender, J
de With, G
and
den Toonder, J.M.J
2000.
Elastic modulus, indentation pressure and fracture toughness of hybrid coatings on glass.
Thin Solid Films,
Vol. 366,
Issue. 1-2,
p.
139.
Lemoine, P.
Zhao, J.F.
Quinn, J.P.
McLaughlin, J.A.
and
Maguire, P.
2000.
Hardness measurements at shallow depths on ultra-thin amorphous carbon films deposited onto silicon and Al2O3–TiC substrates.
Thin Solid Films,
Vol. 379,
Issue. 1-2,
p.
166.
Lemoine, P
Zhao, J.F
Quinn, J.P
Ogwu, A.A
McLaughlin, J.A
Maguire, P
McGinnity, F
and
Shi, X
2000.
Naniondentation and scratch resistance testing on magnetic tape heads coated with ultra-thin amorphous carbon layers.
Wear,
Vol. 244,
Issue. 1-2,
p.
79.
Abdul-Baqi, A.
and
Van der Giessen, E.
2001.
Delamination of a strong film from a ductile substrate during indentation unloading.
Journal of Materials Research,
Vol. 16,
Issue. 5,
p.
1396.
Lim, Yong Yee
and
Chaudhri, M Munawar
2001.
Do residual nano indentations in metals and ceramics relax with time?.
Journal of Physics D: Applied Physics,
Vol. 34,
Issue. 13,
p.
L70.
Chaudhri, M. Munawar
2001.
A note on a common mistake in the analysis of nanoindentation data.
Journal of Materials Research,
Vol. 16,
Issue. 2,
p.
336.
Veprek, Stan
and
Argon, Ali S.
2002.
Towards the understanding of mechanical properties of super- and ultrahard nanocomposites.
Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena,
Vol. 20,
Issue. 2,
p.
650.
Lim, Y.Y.
and
Chaudhri, M.M.
2002.
Nanohardness Mapping of the Curved Surface of Spherical Macroindentations in Fully Annealed Polycrystalline Oxygen-Free Copper.
physica status solidi (a),
Vol. 194,
Issue. 1,
p.
19.
Banini, G. K.
Nazarova, T. A.
Hangen, U. D.
Landwehr, K.
Tymiak, N.
Lim, Y. Y.
and
Chaudhri, M. M.
2002.
Nanoindentation around Vickers microindentation in MgO (100) crystal.
Zeitschrift für Metallkunde,
Vol. 93,
Issue. 9,
p.
875.
Ye, Jiping
Kano, Makoto
and
Yasuda, Yoshiteru
2002.
Evaluation of Local Mechanical Properties in Depth in MoDTC/ZDDP and ZDDP Tribochemical Reacted Films Using Nanoindentation.
Tribology Letters,
Vol. 13,
Issue. 1,
p.
41.
Hernandez, Carmen M.
Murray, Todd W.
and
Krishnaswamy, Sridhar
2002.
Photoacoustic characterization of the mechanical properties of thin films.
Applied Physics Letters,
Vol. 80,
Issue. 4,
p.
691.
Abdul-Baqi, A.
and
Van der Giessen, E.
2002.
Numerical analysis of indentation-induced cracking of brittle coatings on ductile substrates.
International Journal of Solids and Structures,
Vol. 39,
Issue. 6,
p.
1427.
Lonardo, P.M.
Lucca, D.A.
and
De Chiffre, L.
2002.
Emerging Trends in Surface Metrology.
CIRP Annals,
Vol. 51,
Issue. 2,
p.
701.
Miyahara, K.
Nagashima, N.
and
Matsuoka, S.
2002.
Development and application of a combined atomic force microscopy-nanoindentation system with a silicon tip and a diamond indenter.
Philosophical Magazine A,
Vol. 82,
Issue. 10,
p.
2149.
Algueró, M.
Bushby, A. J.
Reece, M. J.
and
Seifert, A.
2002.
Anelastic deformation of Pb(Zr,Ti)O3 thin films by non-180° ferroelectric domain wall movements during nanoindentation.
Applied Physics Letters,
Vol. 81,
Issue. 3,
p.
421.
Tsui, Ting Y.
Ross, C. A.
and
Pharr, G. M.
2003.
A method for making substrate-independent hardness measurements of soft metallic films on hard substrates by nanoindentation.
Journal of Materials Research,
Vol. 18,
Issue. 6,
p.
1383.
Barbour, Michele E.
Parker, David M.
and
Jandt, Klaus D.
2003.
Enamel dissolution as a function of solution degree of saturation with respect to hydroxyapatite: a nanoindentation study.
Journal of Colloid and Interface Science,
Vol. 265,
Issue. 1,
p.
9.
Lim†, Yong Yee
and
Chaudhri‡, M. Munawar
2003.
Experimental investigations of the normal loading of elastic spherical and conical indenters on to elastic flats.
Philosophical Magazine,
Vol. 83,
Issue. 30,
p.
3427.
Barbour, Michele E.
Parker, David M.
Allen, Geoff C.
and
Jandt, Klaus D.
2003.
Human enamel dissolution in citric acid as a function of pH in the range 2.30≤pH≤6.30 – a nanoindentation study.
European Journal of Oral Sciences,
Vol. 111,
Issue. 3,
p.
258.