Hostname: page-component-857557d7f7-c8jtx Total loading time: 0 Render date: 2025-11-20T20:20:48.717Z Has data issue: false hasContentIssue false

X-ray Fractography on Fatigue Fractured Surface of Austenitic Stainless Steel

Published online by Cambridge University Press:  06 March 2019

Zenjiro Yajima
Affiliation:
Department of Mechanical Engineering, Kanazawa Institute of Technology 7-1 Oogigaoka, Nonoichi, Kanazawa 921, Japan
Hideki Tokuyama
Affiliation:
Graduate School, Kanazawa Institute of Technology 7-1 Oogigaoka, Nonoichi, Kanazawa 921, Japan
Yasuo Kibayashi
Affiliation:
Department of Materials Science, Kanazawa University Kakuma-machi, Kanazawa 920-11, Japan
Yukio Hirose
Affiliation:
Department of Materials Science, Kanazawa University Kakuma-machi, Kanazawa 920-11, Japan
Get access

Extract

X-ray diffraction observation of the material internal structure beneath fracture surfaces provide fracture analysis with useful information to investigate the conditions and mechanisms of fracture. X-ray fractography is a generic name given to this technique.

In the present study, X-ray fractography was applied to fatigue fracture surfaces of austenitic stainless steel (AISI 304) which consisted of solution treatment. The fatigue tests were carried out on compact tension (CT) specimens. The plastic strain on the fracture surface was estimated from measuring the line broadening of X-ray diffraction profiles. The line broadening of X-ray diffraction profiles was measured on and beneath fatigue fracture surfaces. The depth of the plastic zone left on fracture surfaces was evaluated from the line broadening. The results are discussed on the basis of fracture mechanics.

Information

Type
V. Residual Stress, Crystallite Size and rms Strain Determination by Diffraction Methods
Copyright
Copyright © International Centre for Diffraction Data 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Yajima, Z., Hirose, Y., and Tanaka, K., “X-Ray Examination of Fracture Surfaces of Silicon Nitride Ceramics,” Advances in X-Ray Analysis, 33: 319(1990).Google Scholar
2. Yajima, Z., Shimazu, Y., Ishikawa, K., Hirose, Y., and Tanaka, K., “X-Ray Fractographic study on Fracture Surface Made by Fatigue Crack Propagation Tests of Ductile Cast Iron,Journal of The Japanese Society for Strength and Fracture of Materials, 22: 121(1988).Google Scholar
3. Yajjma, Z., Hirose, Y., and Tanaka, K., “X-Ray Fractography of Fatigue Fracture of Low-Alloy Steel in Air and in 3.5% NaCl Solution,Journal of The Society of Materials Science Japan, 35: 725(1986).Google Scholar
4. Yajjma, Z., Hirose, Y., and Tanaka, K., “Fracture Toughness and X-Ray Diffraction Observation of Fracture Surface of Ductile Cast Iron,Mechanical Behaviour of Materiak-IV, 1CM4, 2: 725(1983).Google Scholar
5. Yajima, Z., Hirose, Y., and Tanaka, K., “X-Ray Diffraction Observation of Fracture Surfaces of Ductile Cast Iron,” Advances in X-Ray Analysis, 26:291(1983).Google Scholar
6. Tanaka, K., and Akiniwa, Y., “X-Ray Examination of Fatigue Fracture Surface for Failure Analysis,” Role of Fracture Mechanics in Modern Technology, 735(1987).Google Scholar
7. Yajima, Z., Tokuyama, H., and Hirose, Y., “A Study on The Application of X-Ray Diffraction Technique to Fracture Analysis of Austenitic Stainless Steel,” To be published in Journal of The Japanese Society for Strength and Fracture of Materials. Google Scholar
8. Yajima, Z., Hirose, Y., Tanaka, K., and Ogawa, H., “X-Ray Fractographic Study on Fracture Toughness of Ductile Cast Iron at Low Temperatures,” Journal of The Society of Materials Science Japan, 32:1345(1983).Google Scholar
9. Kikukawa, M., Jono, M., Tanaka, K., and Takatani, M., “Measurement of Fatigue Crack Propagation and Crack Closure at Low Stress Intensity Level by Unloading Elastic Compliance Method,” Journal of The Society of Materials Science Japan, 25:899(1976).Google Scholar
10. Levy, N., Marcal, P. V., Ostengren, W. J., and Rice, J. R., “Small Scale Yielding Near A Crack in Plane Strain: A Finite Element Analysis,International Journal of Fracture, 7: 143(1971).Google Scholar